Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of FORTRON® LM1140L4 - PPS-GF40 - Celanese

Material Data Center offers the following functions for FORTRON® LM1140L4:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Fortron datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Fortron LM1140L4 is a 40% glass-reinforced grade that is the strongest and toughest product available. It is laser markable.  It exhibits excellent heat and chemical resistance, good electrical properties and is inherently flame-retardant. The high hardness and rigidity at elevated temperatures allows for good load bearing performance. This product has good weldability due to the modest filler level. Applications made of this grade are electronical components (i.e. bobbins, lamp housings, brush holders) and various other components requiring strength and resistance to aggressive chemicals (i.e. automotive heaters, pumps, valves, fuel rails, microwave oven rings and distillation column packings).

Flammability @1.6mm nom. thickn.V-0-
Flammability at thickness h (0.38 mm)V-0-
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Ritiro di stampaggio, parallelo 0.3 % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.6 % ISO 294-4, 2577
Capacità termica specifica del fuso 1500 J/(kg K) -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 14700 MPa ISO 527
Carico unitario a rottura 195 MPa ISO 527
Deformazione a rottura 1.9 % ISO 527
Resistenza all'urto Charpy, +23°C 53 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C 53 kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 10 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 10 kJ/m² ISO 179/1eA
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 280 °C ISO 11357-1/-3
Temperatura di transizione vetrosa, 10°C/min 90 °C ISO 11357-1/-2
Temp.di inflessione sotto carico, 1.80 MPa 270 °C ISO 75-1/-2
Temp.di inflessione sotto caricor, 8.00 MPa 215 °C ISO 75-1/-2
Coeff.di dilatazione termica lin., parallelo 26 E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 42 E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm V-0 class IEC 60695-11-10
Spessore provato 1.5 mm -
Reazione al fuoco a spessore h V-0 class IEC 60695-11-10
Spessore provato 0.4 mm -
Reazione al fuoco 5V a spess. h 5VA class IEC 60695-11-20
Spessore provato 3.0 mm -
Indice di ossigeno 47 % ISO 4589-1/-2
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Costante dielettrica relativa, 1MHz 4.1 - IEC 62631-2-1
Fattore di dissipazione, 1MHz 20 E-4 IEC 62631-2-1
Resistività volumica >1E13 Ohm*m IEC 62631-3-1
Resistività superficiale 6.6E11 Ohm IEC 62631-3-2
Rigidità dielettrica 28 kV/mm IEC 60243-1
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'acqua 0.02 % Sim. alla ISO 62
Massa volumica 1650 kg/m³ ISO 1183
Funzioni
Modulo dinamico a taglio-temperatura , FORTRON® LM1140L4, PPS-GF40, Celanese
Sforzi-deformazione , FORTRON® LM1140L4, PPS-GF40, Celanese
Modulo secante-deformazione , FORTRON® LM1140L4, PPS-GF40, Celanese
Sforzi-deformazioni (isocrona) 23°C, FORTRON® LM1140L4, PPS-GF40, Celanese
Modulo di scorrimento-tempo 23°C, FORTRON® LM1140L4, PPS-GF40, Celanese
Curva di scorrimento 23°C, FORTRON® LM1140L4, PPS-GF40, Celanese
Sforzi-deformazioni (isocrona) 120°C, FORTRON® LM1140L4, PPS-GF40, Celanese
Modulo di scorrimento-tempo 120°C, FORTRON® LM1140L4, PPS-GF40, Celanese
Curva di scorrimento 120°C, FORTRON® LM1140L4, PPS-GF40, Celanese
Sforzi-deformazioni (isocrona) 150°C, FORTRON® LM1140L4, PPS-GF40, Celanese
Modulo di scorrimento-tempo 150°C, FORTRON® LM1140L4, PPS-GF40, Celanese
Curva di scorrimento 150°C, FORTRON® LM1140L4, PPS-GF40, Celanese
Sforzi-deformazioni (isocrona) 200°C, FORTRON® LM1140L4, PPS-GF40, Celanese
Modulo di scorrimento-tempo 200°C, FORTRON® LM1140L4, PPS-GF40, Celanese
Curva di scorrimento 200°C, FORTRON® LM1140L4, PPS-GF40, Celanese
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet
Additivi
Agente di distacco
Altre informazioni
Stampaggio ad Iniezione
Predrying in a dehumidified air dryer at 130 - 140 degC/3-4 hours is recommended.
On injection molding machines with 15-25 D long three-section screws, as are usual in the trade, the FORTRON is processable. A shut-off nozzle is preferred to a free-flow nozzle.

Melt temperature 320-340 degC
Mold wall temperature at least 140 degC

A medium injection rate is normally preferred. All mold cavities must be effectively vented.
Tool temperature of at least 135 degC is recommended for parts to achieve maximum crystallizable potential.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.