Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Genestar™ G1300H-F02 - PA9T-GF30 - Kuraray Co., Ltd.

Material Data Center offers the following functions for Genestar™ G1300H-F02:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Genestar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
GENESTAR G1300H-F02 is an injection molding grade with 30% GF developed for reflow applications. It is halogen-free and has a HB flammability.

Thanks to its JEDEC MSL 1 rating (moisture sensitive level 1), this grade shows an excellent resistance to blisters.

GENESTAR G1300H-F02 is suitable for all kind of reflow components such as:
- FPC connectors
- Board-to-board connectors
- wire-to-board connectors
- automotive connectors
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Ritiro di stampaggio, parallelo 0.3 % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 1.0 % ISO 294-4, 2577
ASTM Data
Indice di fluidità a caldo, MFI 45 g/10min ASTM D 1238
Temperatura 320 °C -
Carico 2.16 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 9500 MPa ISO 527
Carico unitario a rottura 151 MPa ISO 527
Deformazione a rottura 1.9 % ISO 527
Resistenzia all'urto Charpy con intaglio, +23°C 11 kJ/m² ISO 179/1eA
ASTM Data
Resistenza alla trazione 160 MPa ASTM D 638
Modulo a flessione 8500 MPa ASTM D 790
Resistenza alla flessione 205 MPa ASTM D 790
Resistenza all'urto Izod con intaglio, 1/8 in 105 J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 306 °C ISO 11357-1/-3
Temperatura di transizione vetrosa, 10°C/min 125 °C ISO 11357-1/-2
Temp.di inflessione sotto carico, 1.80 MPa 290 °C ISO 75-1/-2
Reaz. al fuoco spess.nom. 1.5mm HB class IEC 60695-11-10
ASTM Data
UL 94 combustibilitá HB - UL 94
DTUL a 264 psi 290 °C ASTM D 648
Temperatura di fusione 306 °C ASTM D 3418
Temperatura di transizione vetrosa 125 °C ASTM E 1356
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Rigidità dielettrica 28 kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali 600 - IEC 60112
ASTM Data
Rigidità elettrica, breve periodo di tempo 30 kV/mm ASTM D 149
Resistenza di volume >1E15 Ohm*cm ASTM D 257
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'acqua 0.18 % Sim. alla ISO 62
Massa volumica 1370 kg/m³ ISO 1183
Densità 1370 kg/m³ ASTM D 792
Funzioni
Sforzi-deformazione , Genestar™ G1300H-F02, PA9T-GF30, Kuraray
Modulo secante-deformazione , Genestar™ G1300H-F02, PA9T-GF30, Kuraray
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet
Caratteristiche speciali
Ritardante di fiamma, Senza alogeni, Stabilizzato o stabile al calore
Caratteristiche
Saldabile
Disponibilità geografica
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com