Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of K-Resin® KR38 - SB - INEOS Styrolution

Material Data Center offers the following functions for K-Resin® KR38:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other K-Resin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
K-Resin® KR38 alone or in blends, can be easily processed by extrusion and gives thermoformed parts with excellent detail on fast production cycles. The favorable economics of K-Resin SBC, along with high productivity, have made possible tough clear disposable drinking cups, lids, IC carrier tape and other packaging applications.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 9 cm³/10min ISO 1133
Temperatura 200 °C -
Carico 5 kg -
Indice di Fluiditá, MFI 9 g/10min ISO 1133
Temperatura 200 °C -
Carico 5 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 900 MPa ISO 527
Carico unitario a trazione 16.2 MPa ISO 527
Deformazione a rottura >50 % ISO 527
Modulo a flessione, 23°C 1360 MPa ISO 178
Resistenza all'urto Charpy, +23°C N kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 50 kJ/m² ISO 179/1eA
Durezza Shore D 56 - ISO 7619-1
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 55 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 73 °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 50 °C ISO 306
ASTM Data
Temp.di rammollimento Vicat 74.4 °C ASTM D 1525
Proprietà OtticheValoreUnitáNorma del test
ASTM Data
Trasmissione luminosa 92 % ASTM D 1003
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'umidità 0.07 % Sim. alla ISO 62
Massa volumica 1000 kg/m³ ISO 1183
Caratteristiche
Processabilità e Forma di Forni
Estrusione di Lastre/Fogli, Soffiaggio, Termoformatura
Forma fisica disponibile
Pellet
Caratteristiche speciali
Trasparente
Caratteristiche
Miscela di resina, High Gloss, Copolimero
Certifications
Contatto con acqua potabile
Applicazioni
Imballaggio
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Altre informazioni
Stampaggio ad Iniezione
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.