Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kynar® Film 252 PGM TR - PVDF - ARKEMA

Material Data Center offers the following functions for Kynar® Film 252 PGM TR:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kynar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
is a flexible thermoplastic fluorinated film. The properties are the same as standard grade: chemical resistance, resistance to UV, low permeation, high purity, excellent mechanical behavior. These films are specially designed for photovoltaic applications.
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Rigidità dielettrica 100 kV/mm IEC 60243-1
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'umidità 0.2 % Sim. alla ISO 62
Massa volumica 1400 kg/m³ ISO 1183
Proprietà Meccaniche (Film)ValoreUnitáNorma del test
ISO Data
Carico allo snervamento, parallelo 30 MPa ISO 527-3
Carico allo snervamento, perpend. 30 MPa ISO 527-3
Allungamento allo snervamento, parallelo 7 % ISO 527-3
Allungamento allo snervamento, perpend. 7 % ISO 527-3
Carico massimo, parallelo 30 MPa ISO 527-3
Carico massimo, perpend. 30 MPa ISO 527-3
Allungamento massimo, parallelo 150 % ISO 527-3
Allungamento massimo, perpend. 150 % ISO 527-3
Resistenza alla lacerazione Trouser, parallelo 2 N/mm ISO 6383-1
Resistenza alla lacerazione Trouser, perpend. 3 N/mm ISO 6383-1
Tipo di estrusione blown - -
Spessore del provino 0.025 mm -
Caratteristiche
Caratteristiche speciali
Stabilizzato o stabile alla luce, Estab. agli U.V. o per applicaz.in esterni
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Resistenza chimica
Acidi
Acido acetico (5% da massa) (23°C)
Soluzione acida citrica (10% da massa) (23°C)
Acido lattico (10% da massa) (23°C)
Acido cloridrico (36% da massa) (23°C)
Acido nitrico (40% da massa) (23°C)
Acido solforico (38% da massa) (23°C)
Acido solforico (5% da massa) (23°C)
Soluzione acida cromica (40% da massa) (23°C)
Basi
Soluzione dell' idrossido del sodio (35% da massa) (23°C)
Soluzione dell' idrossido del sodio (1% da massa) (23°C)
Soluzione dell' idrossido di ammonio (10% da massa) (23°C)
Alcool
Alcool di isopropile (23°C)
Metanolo (23°C)
Etanolo (23°C)
Idrocarburi
n-Hexane (23°C)
Toluene (23°C)
isoottano (23°C)
Chetoni
Acetone (23°C)
Eteri
Etere Etilico (23°C)
Oli minerali
Olio multigrade del motore di SAE 10W40 (23°C)
Olio multigrade del motore di SAE 10W40 (130°C)
Olio dell' ipoide-ingranaggio di SAE 80/90 (130°C)
Olio isolante (23°C)
Combustibili Standard
Liquido 1 di ISO 1817 (60°C)
Liquido 2 di ISO 1817 (60°C)
Liquido 3 di ISO 1817 (60°C)
Liquido 4 di ISO 1817 (60°C)
Combust. stand. senza alcool (pref. ISO 1817 liquido C) (23°C)
Combust. stand. con alcool (pref. ISO 1817 liquido 4) (23°C)
Combustibile diesel (pref. ISO 1817 liquido F) (23°C)
Combustibile diesel (pref. ISO 1817 liquido F) (90°C)
Combustibile diesel (pref. ISO 1817 liquido F) (>90°C)
Soluzioni saline
Soluzione del cloruro di sodio (10% da massa) (23°C)
Soluzione dell' ipoclorito del sodio (10% da massa) (23°C)
Soluzione del carbonato di sodio (20% da massa) (23°C)
Soluzione del carbonato di sodio (2% da massa) (23°C)
Soluzione del cloruro dello zinco (50% da massa) (23°C)
Altri
Acetato etilico (23°C)
Perossido di idrogeno (23°C)
Glicol etilenico (50% da massa) in acqua (108°C)
Acqua (23°C)
Acqua deionizzata (90°C)
Soluzione del fenolo (5% da massa) (23°C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.