Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LASTILAC AR-V0E - ABS - LATI Industria Termoplastici S.p.A.

Material Data Center offers the following functions for LASTILAC AR-V0E:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lastil datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Ritiro di stampaggio, parallelo 0.5 % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.6 % ISO 294-4, 2577
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 2300 MPa ISO 527
Carico unitario a trazione 40 MPa ISO 527
Deformazione a snervamento 2 % ISO 527
Carico unitario a rottura 35 MPa ISO 527
Deformazione a rottura 8 % ISO 527
Resistenza all'urto Charpy, +23°C 50 kJ/m² ISO 179/1eU
Resist. urto Charpy con intaglio, +23°C 7 kJ/m² ISO 179/1eA
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 80 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 85 °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 95 °C ISO 306
Coeff.di dilatazione termica lin., parallelo 70 E-6/K ISO 11359-1/-2
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (1) 1 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (2) 2 mm -
Glow Wire Ignition Temperature (GWIT) 850 °C IEC 60695-2-13
GWIT - thickness tested (1) 1 mm -
Glow Wire Ignition Temperature (GWIT) 725 °C IEC 60695-2-13
GWIT - thickness tested (2) 2 mm -
ASTM Data
UL 94 combustibilitá V-2 - UL 94
Spessore testati 0.75 mm -
Indice limite di ossigeno 28 % ASTM D 2863
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Res. Alle correnti striscianti superficiali 350 - IEC 60112
ASTM Data
Resistenza superficiale 1E12 Ohm ASTM D 257
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1200 kg/m³ ISO 1183
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 70 - 80 °C -
Pre-essiccamento - Tempo 3 h -
Temperatura di fusione 180 - 210 °C -
Temperatura dello stampo 40 - 60 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Additivi
Agente ritardante di fiamma
Caratteristiche
Copolimero
Disponibilità geografica
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.