Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LUPOY SP2101F - (PC+SI)-GF10 - LG Chem

Material Data Center offers the following functions for LUPOY SP2101F:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lupoy datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di Fluiditá, MFI 10 g/10min ISO 1133
Temperatura 300 °C -
Carico 1.2 kg -
Ritiro di stampaggio, parallelo 0.6 % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.6 % ISO 294-4, 2577
ASTM Data
Indice di fluidità a caldo, MFI 10 g/10min ASTM D 1238
Temperatura 300 °C -
Carico 1.2 kg -
Ritiro di stampaggio, parallelo 0.006 mm/mm ASTM D 955
Ritiro di stampaggio, perpend. 0.006 mm/mm ASTM D 955
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 3570 MPa ISO 527
Carico unitario a trazione 50 MPa ISO 527
Deformazione a snervamento 5 % ISO 527
Carico unitario a rottura 48 MPa ISO 527
Deformazione a rottura 8 % ISO 527
Modulo a flessione, 23°C 3100 MPa ISO 178
Resistenza alla flessione 85 MPa ISO 178
Resist. urto Charpy con intaglio, +23°C 17[1] kJ/m² ISO 179/1eA
Resist. urto Charpy con intaglio, -30°C 9[1] kJ/m² ISO 179/1eA
Resistenza all'urto Izod con intaglio, +23°C 15[1] kJ/m² ISO 180/1A
Resistenza all'urto Izod con intaglio 7[1] kJ/m² ISO 180/1A
Temperatura -40 °C -
Durezza Rockwell R 120 - ISO 2039-2
ASTM Data
Modulo a trazione 3897 MPa ASTM D 638
Resistenza alla trazione di snervamento 54 MPa ASTM D 638
Resistenza alla trazione a rottura 45.1 MPa ASTM D 638
Allungamento a snervamento 5 % ASTM D 638
Allungamento a rottura 18 % ASTM D 638
Modulo a flessione 2845 MPa ASTM D 790
Resistenza alla flessione 93.2 MPa ASTM D 790
Durezza Rockwell R 120 - ASTM D 785
Resistenza all'urto Izod con intaglio, 1/8 in 196 J/m ASTM D 256
Resistenza all'urto Izod con intaglio, 1/4 in 137 J/m ASTM D 256
Resistenza all'urto Izod con intaglio, basso temperatura 88.3 J/m ASTM D 256
Temperatura -30 °C -
1: 4 mm
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 122[2] °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 134[2] °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 138 °C ISO 306
Coeff.di dilatazione termica lin., parallelo 48 E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin. , perpend. 77 E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm V-0 class IEC 60695-11-10
Spessore provato 1.5 mm -
Reazione al fuoco a spessore h V-1 class IEC 60695-11-10
Spessore provato 1.0 mm -
ASTM Data
UL 94 combustibilitá HB - UL 94
Spessore testati 0.8 mm -
coefficiente d’espansione termica, lung. 48 E-6/K ASTM D 696
Coefficiente d’espansione termica, tras. 77 E-6/K ASTM D 696
DTUL a 66 psi 134[3] °C ASTM D 648
DTUL a 264 psi 121[3] °C ASTM D 648
Temp.di rammollimento Vicat 138 °C ASTM D 1525
2: 4 mm  3: 6.4 mm
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Resistività volumica 1E15 Ohm*m IEC 62631-3-1
Resistività superficiale 1E15 Ohm IEC 62631-3-2
ASTM Data
Rigidità elettrica, breve periodo di tempo 19 kV/mm ASTM D 149
Resistenza superficiale 1E15 Ohm ASTM D 257
Resistenza di volume 1E17 Ohm*cm ASTM D 257
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'umidità 0.2 % Sim. alla ISO 62
Massa volumica 1240 kg/m³ ISO 1183
Densità 1240 kg/m³ ASTM D 792
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 95 - 105 °C -
Pre-essiccamento - Tempo 3 - 5 h -
Umidità del Processo ≤0.02 % -
Temperatura di fusione 235 - 265 °C -
Temperatura dello stampo 80 - 120 °C -
Zona 1 260 - 275 °C -
Zona 2 270 - 285 °C -
Zona 3 280 - 295 °C -
Temperatura dell ugello 270 - 285 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Caratteristiche speciali
Ritardante di fiamma, Senza alogeni, Alto urto o modificato all'urto
Applicazioni
Elettrotecnica ed electrici, Polivalente
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com