Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® 378P - SAN - INEOS Styrolution

Material Data Center offers the following functions for Luran® 378P:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Easy-flow grade with enhanced resistance to chemicals.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 20 cm³/10min ISO 1133
Temperatura 220 °C -
Carico 10 kg -
Densità del fuso 970 kg/m³ -
Conduttività termica del fuso 0.17 W/(m K) -
Capacità termica specifica del fuso 2300 J/(kg K) -
Temperatura di estrazione 98 °C -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 3800 MPa ISO 527
Carico unitario a rottura 75 MPa ISO 527
Deformazione a rottura 3.5 % ISO 527
Modulo di scorrimento a trazione, 1h 3500 MPa ISO 899-1
Modulo di scorrimento a trazione, 1000h 2800 MPa ISO 899-1
Resistenza all'urto Charpy, +23°C 19 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C 19 kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 2 kJ/m² ISO 179/1eA
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 89 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 101 °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 107 °C ISO 306
Coeff.di dilatazione termica lin., parallelo 70 E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm HB class IEC 60695-11-10
Spessore provato 1.6 mm -
Yellow Card disponibile - -
Indice di ossigeno 18 % ISO 4589-1/-2
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 3 - IEC 62631-2-1
Costante dielettrica relativa, 1MHz 2.7 - IEC 62631-2-1
Fattore di dissipazione, 100Hz 50 E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 80 E-4 IEC 62631-2-1
Resistività volumica >1E13 Ohm*m IEC 62631-3-1
Resistività superficiale >1E15 Ohm IEC 62631-3-2
Res. Alle correnti striscianti superficiali 425 - IEC 60112
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'umidità 0.3 % Sim. alla ISO 62
Massa volumica 1080 kg/m³ ISO 1183
Preparazione ProvetteValoreUnitáNorma del test
ISO Data
Stamp. ad Iniezione, temp. di fusione 230 °C ISO 294
Stamp. ad Iniezione, temperatura dello stampo 50 °C ISO 294
Stamp. ad Iniezione, velocità media d'iniezione 200 mm/s ISO 294
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 80 °C -
Pre-essiccamento - Tempo 2 - 4 h -
Temperatura di fusione 220 - 260 °C -
Temperatura dello stampo 40 - 80 °C -
Funzioni
Viscosità-Velocità di taglio , Luran® 378P, SAN, INEOS Styrolution
Sforzo di taglio-Velocità di taglio , Luran® 378P, SAN, INEOS Styrolution
Modulo dinamico a taglio-temperatura , Luran® 378P, SAN, INEOS Styrolution
Sforzi-deformazione , Luran® 378P, SAN, INEOS Styrolution
Modulo secante-deformazione , Luran® 378P, SAN, INEOS Styrolution
Sforzi-deformazioni (isocrona) 23°C, Luran® 378P, SAN, INEOS Styrolution
Modulo di scorrimento-tempo 23°C, Luran® 378P, SAN, INEOS Styrolution
Curva di scorrimento 23°C, Luran® 378P, SAN, INEOS Styrolution
Sforzi-deformazioni (isocrona) 40°C, Luran® 378P, SAN, INEOS Styrolution
Modulo di scorrimento-tempo 40°C, Luran® 378P, SAN, INEOS Styrolution
Curva di scorrimento 40°C, Luran® 378P, SAN, INEOS Styrolution
Sforzi-deformazioni (isocrona) 60°C, Luran® 378P, SAN, INEOS Styrolution
Modulo di scorrimento-tempo 60°C, Luran® 378P, SAN, INEOS Styrolution
Curva di scorrimento 60°C, Luran® 378P, SAN, INEOS Styrolution
Sforzi-deformazioni (isocrona) 80°C, Luran® 378P, SAN, INEOS Styrolution
Modulo di scorrimento-tempo 80°C, Luran® 378P, SAN, INEOS Styrolution
Curva di scorrimento 80°C, Luran® 378P, SAN, INEOS Styrolution
Volume specifico-temperatura (pvT) , Luran® 378P, SAN, INEOS Styrolution
Modulo a taglio-temperatura , Luran® 378P, SAN, INEOS Styrolution
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet
Caratteristiche speciali
Trasparente
Disponibilità geografica
Altre informazioni
Stampaggio ad Iniezione
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 2 - 4 h

PROCESSING
injection molding, Melt temperature, range: 220 - 260 °C
injection molding, Melt temperature, recommended: 250 °C
injection molding, Mold temperature, range: 40 - 80 °C
injection molding, Mold temperature, recommended: 50 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.