Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® ECO 348Q BC80 - SAN - INEOS Styrolution

Material Data Center offers the following functions for Luran® ECO 348Q BC80:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Luran® ECO 348Q is a grade of SAN, suitable for moldings with very thin walls and / or adverse flow length to wall ratio. It features excellent transparency and a light intrinsic color. Luran ECO 348Q BC80 is an ISCC compliant product leading to a substitution of fossil source styrene with ISCC certified bio-attributed styrene.
Carbon Footprint Reduction vs Fossil-Based (3rd party validated): 99 % (ISO 14044)
Attributed Content of ISCC-certified Bio-Circular Sources (min.): 80 %
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 19 cm³/10min ISO 1133
Temperatura 220 °C -
Carico 10 kg -
Ritiro di stampaggio, parallelo 0.5 % ISO 294-4, 2577
Conduttività termica del fuso 0.17 W/(m K) -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 3600 MPa ISO 527
Carico unitario a rottura 70 MPa ISO 527
Deformazione a rottura 2.5 % ISO 527
Modulo a flessione, 23°C 3400 MPa ISO 178
Resistenza alla flessione 115 MPa ISO 178
Resistenza all'urto Charpy, +23°C 14 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C 14 kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 1.5 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 1.5 kJ/m² ISO 179/1eA
Resistenza all'urto Izod con intaglio, +23°C 1.5 kJ/m² ISO 180/1A
Ball indentation hardness 160 MPa ISO 2039-1
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 99 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 99 °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 105 °C ISO 306
Coeff.di dilatazione termica lin., parallelo 70 E-6/K ISO 11359-1/-2
Other Standards[S]
Conduttività termica, stato solido 0.17 W/(m K) DIN 52612-1
S: These properties are reported by the producer according standards that are different to our defaults.
Proprietà OtticheValoreUnitáNorma del test
ASTM Data
Opacità 1 % ASTM D 1003
Trasmissione luminosa 89 % ASTM D 1003
Other Standards[S]
Indice di rifrazione 1.57 - ISO 489
S: These properties are reported by the producer according standards that are different to our defaults.
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'umidità 0.2 % Sim. alla ISO 62
Massa volumica 1080 kg/m³ ISO 1183
Bulk density 600 kg/m³ -
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 80 °C -
Pre-essiccamento - Tempo 2 - 4 h -
Temperatura di fusione 200 - 250 °C -
Temperatura dello stampo 40 - 80 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet
Caratteristiche speciali
Stabilizzato o stabile al calore, Trasparente
Resistenza Chimica
Resistenza chimica generale
Certifications
Contiene risorse rinnovabili, Contatto con gli alimenti, ISCC Plus
Applicazioni
Imballaggio
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, Near East/Africa
Altre informazioni
Stampaggio ad Iniezione
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature, range: 200 - 250°C

Mold temperature, range: 40 - 80°C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.