Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® HD-20 - SAN - INEOS Styrolution

Material Data Center offers the following functions for Luran® HD-20:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Luran® HD 20 is an easy-flow grade of SAN especially designed for the medical market. It is suitable for moldings with very thin walls and / or adverse flow length to wall ratio. It features very good transparency and a light intrinsic color. Food contact statements are available on request.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 22 cm³/10min ISO 1133
Temperatura 220 °C -
Carico 10 kg -
Conduttività termica del fuso 0.17 W/(m K) -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 3700 MPa ISO 527
Carico unitario a rottura 72 MPa ISO 527
Deformazione a rottura 3 % ISO 527
Resistenza all'urto Charpy, +23°C 16 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C 16 kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 2 kJ/m² ISO 179/1eA
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 86 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 99 °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 106 °C ISO 306
Coeff.di dilatazione termica lin., parallelo 70 E-6/K ISO 11359-1/-2
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 3 - IEC 62631-2-1
Fattore di dissipazione, 100Hz 40 E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 70 E-4 IEC 62631-2-1
Resistività volumica >1E13 Ohm*m IEC 62631-3-1
Resistività superficiale >1E15 Ohm IEC 62631-3-2
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'umidità 0.2 % Sim. alla ISO 62
Massa volumica 1080 kg/m³ ISO 1183
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 80 °C -
Pre-essiccamento - Tempo 2 - 4 h -
Temperatura di fusione 220 - 260 °C -
Temperatura dello stampo 40 - 80 °C -
Funzioni
Viscosità-Velocità di taglio , Luran® HD-20, SAN, INEOS Styrolution
Sforzo di taglio-Velocità di taglio , Luran® HD-20, SAN, INEOS Styrolution
Sforzi-deformazione , Luran® HD-20, SAN, INEOS Styrolution
Modulo secante-deformazione , Luran® HD-20, SAN, INEOS Styrolution
Sforzi-deformazioni (isocrona) 23°C, Luran® HD-20, SAN, INEOS Styrolution
Modulo di scorrimento-tempo 23°C, Luran® HD-20, SAN, INEOS Styrolution
Curva di scorrimento 23°C, Luran® HD-20, SAN, INEOS Styrolution
Sforzi-deformazioni (isocrona) 40°C, Luran® HD-20, SAN, INEOS Styrolution
Modulo di scorrimento-tempo 40°C, Luran® HD-20, SAN, INEOS Styrolution
Curva di scorrimento 40°C, Luran® HD-20, SAN, INEOS Styrolution
Sforzi-deformazioni (isocrona) 60°C, Luran® HD-20, SAN, INEOS Styrolution
Modulo di scorrimento-tempo 60°C, Luran® HD-20, SAN, INEOS Styrolution
Curva di scorrimento 60°C, Luran® HD-20, SAN, INEOS Styrolution
Sforzi-deformazioni (isocrona) 80°C, Luran® HD-20, SAN, INEOS Styrolution
Modulo di scorrimento-tempo 80°C, Luran® HD-20, SAN, INEOS Styrolution
Curva di scorrimento 80°C, Luran® HD-20, SAN, INEOS Styrolution
Volume specifico-temperatura (pvT) , Luran® HD-20, SAN, INEOS Styrolution
Modulo a taglio-temperatura , Luran® HD-20, SAN, INEOS Styrolution
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet
Caratteristiche speciali
Trasparente, Sterilizzabile, Sterilizzazione ad ossido di etilene (EtO), Gamma irradiation sterilization
Resistenza Chimica
Resistenza alla radiazione
Certifications
Contatto con gli alimenti, Approvato per l'utilizzo per contatto con alimenti 10/2011, Approvato per l'utilizzo per contatto con alimenti secondo la FDA 21 CFR, Grado medico, Biocompatibility ISO 10993, Approvazione della USP class VI, Drug Master File, Long term supply assurance
Applicazioni
Medicale
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Altre informazioni
Stampaggio ad Iniezione
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature, range: 220 - 260°C

Mold temperature, range: 40 - 80°C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com