Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of MAGNUM™ 3404 - ABS - Trinseo

Material Data Center offers the following functions for MAGNUM™ 3404:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Magnum datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 6.7 cm³/10min ISO 1133
Temperatura 220 °C -
Carico 10 kg -
Indice di Fluiditá, MFI 6.6 g/10min ISO 1133
Temperatura 220 °C -
Carico 10 kg -
Ritiro di stampaggio, parallelo 0.6 % ISO 294-4, 2577
ASTM Data
Indice di fluidità a caldo, MFI 1.9 g/10min ASTM D 1238
Temperatura 220 °C -
Carico 5 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 2150 MPa ISO 527
Carico unitario a trazione 43 MPa ISO 527
Deformazione a snervamento 2.7 % ISO 527
Modulo a flessione, 23°C 2100 MPa ISO 178
Resistenza alla flessione 70 MPa ISO 178
Resist. urto Charpy con intaglio, +23°C 18 kJ/m² ISO 179/1eA
Resist. urto Charpy con intaglio, -30°C 13 kJ/m² ISO 179/1eA
Resistenza all'urto Izod con intaglio, +23°C 19 kJ/m² ISO 180/1A
Resistenza all'urto Izod con intaglio 11 kJ/m² ISO 180/1A
Temperatura -30 °C -
ASTM Data
Modulo a trazione 2100 MPa ASTM D 638
Resistenza alla trazione di snervamento 46 MPa ASTM D 638
Allungamento a snervamento 4.1 % ASTM D 638
Modulo a flessione 2520 MPa ASTM D 790
Resistenza all'urto Izod con intaglio, 1/8 in 230 J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 101[ann.] °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 102 °C ISO 306
Reaz. al fuoco spess.nom. 1.5mm HB class IEC 60695-11-10
Spessore provato 1.5 mm -
Reazione al fuoco a spessore h HB class IEC 60695-11-10
Spessore provato 3.0 mm -
ASTM Data
Temp.di rammollimento Vicat 102 °C ASTM D 1525
ann.: annealed
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1050 kg/m³ ISO 1183
Densità 1050 kg/m³ ASTM D 792
Caratteristiche
Processabilità e Forma di Forni
Estrusione di Lastre/Fogli, Altre Estrusioni, Termoformatura
Certifications
Contatto con gli alimenti, Approvato per l'utilizzo per contatto con alimenti secondo la FDA 21 CFR
Applicazioni
Polivalente
Disponibilità geografica
Nord America, Europa, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com