Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Novodur® E3TZ - ABS - INEOS Styrolution

Material Data Center offers the following functions for Novodur® E3TZ:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Novodur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Novodur® E3TZ acrylonitrile butadiene styrene (ABS) polymer features high surface quality and good impact strength. Novodur® E3TZ is an extrusion grade with high gloss and good surface appearance. It is optimized for processing via thermoforming. Furthermore, food contact statements are available upon request.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 8 cm³/10min ISO 1133
Temperatura 220 °C -
Carico 10 kg -
Ritiro di stampaggio, parallelo 0.6 % ISO 294-4, 2577
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 2550 MPa ISO 527
Carico unitario a trazione 48 MPa ISO 527
Deformazione a snervamento 2.5 % ISO 527
Deformazione nominale a rottura 15 % ISO 527
Modulo a flessione, 23°C 2600 MPa ISO 178
Resistenza alla flessione 75 MPa ISO 178
Resistenza all'urto Charpy, +23°C 150 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C 110 kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 19 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 9 kJ/m² ISO 179/1eA
Ball indentation hardness 110 MPa ISO 2039-1
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 98 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 103 °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 100 °C ISO 306
Coeff.di dilatazione termica lin., parallelo 90 E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm HB class IEC 60695-11-10
Spessore provato 1.5 mm -
Glow Wire Flammability Index (GWFI) 700 °C IEC 60695-2-12
GWFI - thickness tested (1) 2 mm -
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Resistività superficiale 600 Ohm IEC 62631-3-2
Rigidità dielettrica 35 kV/mm IEC 60243-1
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1050 kg/m³ ISO 1183
Raccomandazione de Processabilità EstrusioneValoreUnitáNorma del test
Type of extrusion profile - -
Pre-essiccamento - Temperatura 80 °C -
Pre-essiccamento - Tempo 2 - 4 h -
Temperatura di fusione 215 - 240 °C -
Type of extrusion sheet - -
Pre-essiccamento - Temperatura 80 °C -
Pre-essiccamento - Tempo 2 - 4 h -
Temperatura di fusione 215 - 240 °C -
Caratteristiche
Processabilità e Forma di Forni
Estrusione Profilati, Estrusione di Lastre/Fogli, Altre Estrusioni, Termoformatura
Forma fisica disponibile
Pellet
Caratteristiche speciali
Alto urto o modificato all'urto
Caratteristiche
High Gloss
Certifications
Contatto con gli alimenti
Disponibilità geografica
Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Altre informazioni
Estrusione di Profilati
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Profiles, Melt temperature: 215 - 240°C

Estrusione Lastre/Fogli
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Sheets, Melt temperature: 215 - 240°C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.