Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of OPTIX® CA - 990 CLEAR - PMMA - Plaskolite West, Inc.

Material Data Center offers the following functions for OPTIX® CA - 990 CLEAR:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Optix datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ASTM Data
Indice di fluidità a caldo, MFI 4 g/10min ASTM D 1238
Temperatura 230 °C -
Carico 3.8 kg -
Ritiro di stampaggio, parallelo 0.004 mm/mm ASTM D 955
Proprietà MeccanicheValoreUnitáNorma del test
ASTM Data
Modulo a trazione 2000 MPa ASTM D 638
Resistenza alla trazione 50 MPa ASTM D 638
Resistenza alla flessione 76 MPa ASTM D 790
Resistenza all'urto Izod con intaglio, 1/4 in 55 J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ASTM Data
coefficiente d’espansione termica, lung. 100 E-6/K ASTM D 696
DTUL a 264 psi 79 °C ASTM D 648
Temp.di rammollimento Vicat 112 °C ASTM D 1525
Proprietà OtticheValoreUnitáNorma del test
ASTM Data
Opacità 1.8 % ASTM D 1003
Trasmissione luminosa 91.6 % ASTM D 1003
Altre ProprietàValoreUnitáNorma del test
Densità 1160 kg/m³ ASTM D 792
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Altre Estrusioni
Caratteristiche speciali
Alto urto o modificato all'urto
Disponibilità geografica
Nord America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.