Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Panlite® G-3430R - PC-GF30 - Teijin Chemicals Ltd.

Material Data Center offers the following functions for Panlite® G-3430R:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Panlite datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ASTM Data
Ritiro di stampaggio, parallelo 0.0011 mm/mm ASTM D 955
Ritiro di stampaggio, perpend. 0.004 mm/mm ASTM D 955
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 8000 MPa ISO 527
Carico unitario a rottura 105 MPa ISO 527
Deformazione a rottura 2 % ISO 527
Modulo a flessione, 23°C 7100 MPa ISO 178
Resistenza alla flessione 160 MPa ISO 178
Resistenza all'urto Charpy, +23°C 35 kJ/m² ISO 179/1eU
Resist. urto Charpy con intaglio, +23°C 12 kJ/m² ISO 179/1eA
ASTM Data
Modulo a trazione 7950 MPa ASTM D 638
Resistenza alla trazione a rottura 108 MPa ASTM D 638
Allungamento a rottura 2.5 % ASTM D 638
Resistenza a compressione 130 MPa ASTM D 695
Modulo a flessione 7260 MPa ASTM D 790
Resistenza alla flessione 162 MPa ASTM D 790
Durezza Rockwell M 92 - ASTM D 785
Resistenza all'urto Izod con intaglio, 1/8 in 120 J/m ASTM D 256
Resistenza all'urto Izod con intaglio, 1/4 in 130 J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 148 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 151 °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 153 °C ISO 306
Coeff.di dilatazione termica lin., parallelo 20 E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin. , perpend. 60 E-6/K ISO 11359-1/-2
Reazione al fuoco a spessore h HB class IEC 60695-11-10
Spessore provato 0.4 mm -
ASTM Data
UL 94 combustibilitá V-2 - UL 94
Spessore testati 0.8 mm -
coefficiente d’espansione termica, lung. 20 E-6/K ASTM D 696
Coefficiente d’espansione termica, tras. 56 E-6/K ASTM D 696
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 3.5 - IEC 62631-2-1
Costante dielettrica relativa, 1MHz 3.5 - IEC 62631-2-1
Fattore di dissipazione, 100Hz 10 E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 90 E-4 IEC 62631-2-1
Resistività volumica >1E13 Ohm*m IEC 62631-3-1
Resistività superficiale >1E15 Ohm IEC 62631-3-2
Rigidità dielettrica 35 kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali 175 - IEC 60112
ASTM Data
Rigidità elettrica, breve periodo di tempo 30 kV/mm ASTM D 149
Fattore di dissipazione dielèttrica, 60 Hz 0.0008 - ASTM D 150
Fattore di dissipazione dielèttrica, 1 MHz 0.009 - ASTM D 150
Costante dielèttrica, 60 Hz 3.51 - ASTM D 150
Costante dielèttrica, 1 MHz 3.41 - ASTM D 150
Resistenza di volume 1E16 Ohm*cm ASTM D 257
Resistenza all’arco 100 s ASTM D 495
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1430 kg/m³ ISO 1183
Assorbimento d’acqua, equilibrio 0.12 % ASTM D 570
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 120 °C -
Pre-essiccamento - Tempo >5 h -
Temperatura di fusione 290 - 320 °C -
Temperatura dello stampo 80 - 120 °C -
Funzioni
Fatigue strength , Panlite® G-3430R, PC-GF30, Teijin Chemicals
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet
Caratteristiche
Resistenza al scorrimento
Applicazioni
Elettrotecnica ed electrici
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.