Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Pebax® MH 2030 - TPA - ARKEMA

Material Data Center offers the following functions for Pebax® MH 2030:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Pebax datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Polyether block amide Pebax® MH 2030 resin is a thermoplastic elastomer made of flexible polyether and rigid polyamide.
Pebax® MH 2030 resin is an inherently dissipative polymer and can be dry blended or compounded with an isolative polymer to lower the surface resistivity of the final part.

Refractive index according to an internal method is 1.508.


Main applications:
  • Permanent antistactic additive


Packaging:

This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione - / 80 MPa ISO 527
Durezza Shore D 40 / * - ISO 7619-1
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 200 / * °C ISO 11357-1/-3
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Resistività volumica - / 100000 Ohm*m IEC 62631-3-1
Resistività superficiale * / 1E7 Ohm IEC 62631-3-2
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 120 / * % Sim. alla ISO 62
Assorbimento d'umidità 4.5 / * % Sim. alla ISO 62
Massa volumica 1140 / 1140 kg/m³ ISO 1183
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 70 - 90 °C -
Pre-essiccamento - Tempo 5 - 7 h -
Temperatura di fusione 230 - 260 °C -
Temperatura dello stampo 25 - 60 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Altre Estrusioni
Forma fisica disponibile
Pellet
Caratteristiche speciali
Migliorata conduttività elettrica, Antistatico
Disponibilità geografica
Altre informazioni
Stampaggio ad Iniezione

Processing conditions:

- Typical melt temperature (Min / Recommended / Max): 230°C / 240°C / 260°C.
- Typical mold temperature: 25–60°C.
- Drying time and temperature (only necessary for bags opened for more than two hours): 5-7 hours at 70-90°C.
Altre Estrusioni

Processing conditions:

- Typical melt temperature (Min / Recommended / Max): 230°C / 250°C / 280°C
- Drying time and temperature (only necessary for bags opened for more than two hours): 5-7 hours at 70-90°C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.