Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Platamid® HX 2592 Pellets - PA* - ARKEMA

Material Data Center offers the following functions for Platamid® HX 2592 Pellets:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Platamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Platamid® HX 2592 Pellets
Copolyamide Hot Melt Adhesive / Extrusion Applications

Platamid® HX 2592 is a specialty thermoplastic co-polyamide hot melt adhesive available in pellet form. This low to medium melt viscosity grade is particularly suitable for manufacturing webs, nets, mono- and multi-filaments, and films by extrusion.
Platamid® HX 2592 offers a very good adhesion to various polar substrates (thermoplastics, thermosets, metal natural fibers, and more). In addition,Platamid® HX 2592 also exhibits strong adhesion onto rigid and plasticized PVC as well as ABS, epoxy resin, PU etc. Dense layers of Platamid® HX 2592 are known to have barrier properties against PVC plasticizer migration.
Platamid® HX 2592 is also characterized by a very high content of bio-based carbon (82% according ASTM D6866), making it a bio-based solution to difficult-to-solve bonding problems.



AVAILABLE GRADES
This product is available:
- Dried (HX 2592 T)
- Un-dried (HX 2592 F)
PACKAGING
- Platamid HX 2592 F is delivered in 25 kg sealed bags and in 500 kg Big Bag
- Platamid HX 2592 T is delivered in 25 kg sealed bags
These grades are ready to be processed.
SHELF LIFE
Two years from the date of delivery. For any use above this limit, please refer to our technical services.
RENEWABLE CARBON CONTENT 
82% (according ASTM D6866)
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 24 / * cm³/10min ISO 1133
Temperatura 160 / * °C -
Carico 2.16 / * kg -
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 106 / * °C ISO 11357-1/-3
Altre Proprietàsecco/condUnitáNorma del test
Massa volumica 1090 / - kg/m³ ISO 1183
Biobased content 80 % -
Caratteristiche
Processabilità e Forma di Forni
Estrusione Film
Forma fisica disponibile
Pellet
Caratteristiche
Proprietà di barriera, Buona adesione, Copolimero
Certifications
Contiene risorse rinnovabili
Applicazioni
Monofilament, Multifilament
Disponibilità geografica
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.