Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of POLYREX PH-88 - (PS-HI) - Chi Mei Corporation

Material Data Center offers the following functions for POLYREX PH-88:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Polyrex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 5.5 cm³/10min ISO 1133
Temperatura 200 °C -
Carico 5 kg -
Ritiro di stampaggio, parallelo 0.6 % ISO 294-4, 2577
ASTM Data
Indice di fluidità a caldo, MFI 6 g/10min ASTM D 1238
Temperatura 200 °C -
Carico 5 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Carico unitario a trazione 26 MPa ISO 527
Carico unitario a rottura 24 MPa ISO 527
Modulo a flessione, 23°C 2100 MPa ISO 178
Resistenza alla flessione 37 MPa ISO 178
Resist. urto Charpy con intaglio, +23°C 11 kJ/m² ISO 179/1eA
Resist. urto Charpy con intaglio, -30°C 6.5 kJ/m² ISO 179/1eA
Resistenza all'urto Izod con intaglio, +23°C 11 kJ/m² ISO 180/1A
Resistenza all'urto Izod con intaglio 6 kJ/m² ISO 180/1A
Temperatura -30 °C -
ASTM Data
Resistenza alla trazione a rottura 23.5 MPa ASTM D 638
Modulo a flessione 1931 MPa ASTM D 790
Resistenza alla flessione 37.2 MPa ASTM D 790
Durezza Rockwell L 60 - ASTM D 785
Resistenza all'urto Izod con intaglio, 1/8 in 98.2 J/m ASTM D 256
Resistenza all'urto Izod con intaglio, 1/4 in 83.3 J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 74 °C ISO 75-1/-2
Temp.di rammollimento Vicat, A 96 °C ISO 306
Temp.di rammollimento Vicat, B 90 °C ISO 306
Coeff.di dilatazione termica lin., parallelo 45 E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm HB class IEC 60695-11-10
Spessore provato 1.5 mm -
Yellow Card disponibile - -
ASTM Data
UL 94 combustibilitá HB - UL 94
Spessore testati 1.5 mm -
Temp.di rammollimento Vicat 97.8 °C ASTM D 1525
Proprietà ElettricheValoreUnitáNorma del test
ASTM Data
Resistenza all’arco 150 s ASTM D 495
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1030 kg/m³ ISO 1183
Densità 1050 kg/m³ ASTM D 792
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 80 °C -
Pre-essiccamento - Tempo 2 - 3 h -
Temperatura dello stampo 40 - 70 °C -
Temperatura - Zona di Alimentazione 160 - 180 °C -
Zona 1 180 - 200 °C -
Temperatura dell ugello 180 - 200 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Caratteristiche speciali
Alto urto o modificato all'urto, Stabilizzato o stabile al calore
Applicazioni
Elettrotecnica ed electrici, Giocattoli
Disponibilità geografica
Asia Oceano Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.