Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Prisma® 3410 - PP - Braskem

Material Data Center offers the following functions for Prisma® 3410:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Prisma datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di Fluiditá, MFI 10 g/10min ISO 1133
Temperatura 230 °C -
Carico 2.16 kg -
ASTM Data
Indice di fluidità a caldo, MFI 10 g/10min ASTM D 1238
Temperatura 230 °C -
Carico 2.16 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Carico unitario a trazione 29 MPa ISO 527
Deformazione a snervamento 13 % ISO 527
Modulo a flessione, 23°C 1050 MPa ISO 178
Resistenza all'urto Izod con intaglio, +23°C 3.5 kJ/m² ISO 180/1A
Resistenza all'urto Izod con intaglio 1.3 kJ/m² ISO 180/1A
Temperatura -20 °C -
Durezza Rockwell R 82 - ISO 2039-2
ASTM Data
Resistenza alla trazione di snervamento 30 MPa ASTM D 638
Allungamento a snervamento 13 % ASTM D 638
Durezza Rockwell R 83 - ASTM D 785
Resistenza all'urto Izod con intaglio, 1/8 in 45 J/m ASTM D 256
Resistenza all'urto Izod con intaglio, basso temperatura 20 J/m ASTM D 256
Temperatura -20 °C -
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 51 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 85 °C ISO 75-1/-2
Temp.di rammollimento Vicat, A 129 °C ISO 306
ASTM Data
DTUL a 66 psi 80 °C ASTM D 648
DTUL a 264 psi 51 °C ASTM D 648
Temp.di rammollimento Vicat 129 °C ASTM D 1525
Proprietà OtticheValoreUnitáNorma del test
ASTM Data
Opacità 9 % ASTM D 1003
Altre ProprietàValoreUnitáNorma del test
Densità 902 kg/m³ ASTM D 792
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Caratteristiche speciali
Trasparente
Caratteristiche
Copolimero, Copolimero casuale
Disponibilità geografica
Nord America, Europa, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.