Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Provista™ UVI - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Provista™ UVI:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Provista datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto

Eastman Provista™ UVI is a copolymer with an indoor/outdoor UV package added to prevent yellowing caused by  light. Eastman Provista™ copolymer is a resin specifically developed for extrusion into profiles where aesthetics like high clarity and gloss, coupled with design flexibility drive demand. Compared to commonly used materials, Eastman Provista™ copolymer can often run on most standard processing equipment at increased speeds. An extremely high melt strength makes the resin an excellent choice when extruding profiles into complicated shapes.




Proprietà MeccanicheValoreUnitáNorma del test
ASTM Data
Resistenza alla trazione di snervamento 50 MPa ASTM D 638
Resistenza alla trazione a rottura 29 MPa ASTM D 638
Allungamento a snervamento 4 % ASTM D 638
Allungamento a rottura 109 % ASTM D 638
Modulo a flessione 2200 MPa ASTM D 790
Resistenza alla flessione 72 MPa ASTM D 790
Durezza Rockwell R 106 - ASTM D 785
Resistenza all'urto Izod con intaglio, 1/8 in 94 J/m ASTM D 256
Resistenza all'urto Izod con intaglio, basso temperatura 52 J/m ASTM D 256
Temperatura -40 °C -
Resistenza all'urto Izod, 1/8 in N J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ASTM Data
DTUL a 66 psi 67 °C ASTM D 648
DTUL a 264 psi 62 °C ASTM D 648
Temp.di rammollimento Vicat 79 °C ASTM D 1525
Proprietà OtticheValoreUnitáNorma del test
ASTM Data
Brillantezza 171 - ASTM D 2457
Opacità 0.6 % ASTM D 1003
Trasmissione luminosa 90 % ASTM D 1003
Altre ProprietàValoreUnitáNorma del test
Densità 1270 kg/m³ ASTM D 792
Color b 0.61 - CIE
Caratteristiche
Processabilità e Forma di Forni
Estrusione Profilati
Caratteristiche speciali
Stabilizzato o stabile alla luce, Estab. agli U.V. o per applicaz.in esterni, Trasparente
Caratteristiche
High Gloss, Resistenza del fuso, Copolimero
Resistenza Chimica
Resistenza chimica generale
Applicazioni
Imballaggio
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.