Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Pyramid™ KD2000 IM - PEEK - Polymics, Ltd.

Material Data Center offers the following functions for Pyramid™ KD2000 IM:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Pyramid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
For more detailed information, please read our brochure
or contact our representatives in your region.
Proprietà MeccanicheValoreUnitáNorma del test
ASTM Data
Modulo a trazione 3400 MPa ASTM D 638
Resistenza alla trazione 97 MPa ASTM D 638
Allungamento a rottura 30 % ASTM D 638
Modulo a flessione 3400 MPa ASTM D 790
Resistenza alla flessione 145 MPa ASTM D 790
Proprietà TermicheValoreUnitáNorma del test
ASTM Data
UL 94 combustibilitá V-0 - UL 94
Spessore testati 1.6 mm -
coefficiente d’espansione termica, lung. 4.7 E-6/K ASTM D 696
DTUL a 264 psi 150 °C ASTM D 648
Temperatura di fusione 340 °C ASTM D 3418
Indice limite di ossigeno 38 % ASTM D 2863
Proprietà ElettricheValoreUnitáNorma del test
ASTM Data
Rigidità elettrica, breve periodo di tempo 21 kV/mm ASTM D 149
Resistenza superficiale 1E14 Ohm ASTM D 257
Altre ProprietàValoreUnitáNorma del test
Assorbimento d’acqua, 24hr 0.5 % ASTM D 570
Densità 1300 kg/m³ ASTM D 792
Caratteristiche
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.