Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsamid® AECHVO - PA12 - ARKEMA

Material Data Center offers the following functions for Rilsamid® AECHVO:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Rilsamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
ISO 16396 - PA12, KHL, C18-010

Rilsamid® AECHVO resin is a natural polyamide 12. 
This grade is designed for cable coating but is also suitable for extrusion.


Main applications:
  • Wire Sheathing


Packaging:
This grade is delivered dried in sealed packaging (800 kg rigid containers) ready to be processed.


Shelf life:
Two years from date of delivery. For any used above this limit, please refer to our technical services.
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 45 / * cm³/10min ISO 1133
Temperatura 235 / * °C -
Carico 5 / * kg -
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione - / 1200 MPa ISO 527
Carico unitario a trazione - / 38 MPa ISO 527
Deformazione a snervamento - / 6 % ISO 527
Deformazione nominale a rottura - / >50 % ISO 527
Resistenzia all'urto Charpy con intaglio, +23°C - / 7 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C - / 6 kJ/m² ISO 179/1eA
Durezza Shore D 73 / * - ISO 7619-1
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 178 / * °C ISO 11357-1/-3
Altre Proprietàsecco/condUnitáNorma del test
Massa volumica 1010 / 1010 kg/m³ ISO 1183
Caratteristiche
Processabilità e Forma di Forni
Estrusione Film, Estrusione di Lastre/Fogli, Altre Estrusioni, Rivestimento
Forma fisica disponibile
Pellet, Colore naturale
Disponibilità geografica
Altre informazioni
Altre Estrusioni
Processing conditions:

Extrusion temperature

- Typical melt temperature (Min / Recommended / Max) : 240°C / 250°C / 260°C.

- Drying time and temperature (only necessary for containers opened for more than two hours) : 4-8 hours at 80°C.

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com