Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsan® MB 3610 NAT - PA11-I - ARKEMA

Material Data Center offers the following functions for Rilsan® MB 3610 NAT:
unit conversion, PDF datasheet print, comparison with other plastics, parameters for material models, CAE Interfaces

Check here, which other Rilsan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
PA11-P, EHL, 22-002
Rilsan® MB 3610 NAT resin is a polyamide 11 produced from a renewable source. This natural grade is plasticized and specially designed for pneumatic applications. It combines very high flexibility with good impact resistance.



Main applications:
  • Pneumatic tubing

Packaging:
This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 4 / * cm³/10min ISO 1133
Temperatura 235 / * °C -
Carico 5 / * kg -
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione - / 210 MPa ISO 527
Resistenzia all'urto Charpy con intaglio, -30°C - / 10 kJ/m² ISO 179/1eA
Durezza Shore D 53 / * - ISO 7619-1
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 188 / * °C ISO 11357-1/-3
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Resistività volumica 1.9E11 / - Ohm*m IEC 62631-3-1
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 1.1 / * % Sim. alla ISO 62
Assorbimento d'umidità 0.45 / * % Sim. alla ISO 62
Massa volumica 1030 / 1030 kg/m³ ISO 1183
Biobased content 59 % -
Funzioni
Viscosità-Velocità di taglio , Rilsan® MB 3610 NAT, PA11-I, ARKEMA
Sforzo di taglio-Velocità di taglio , Rilsan® MB 3610 NAT, PA11-I, ARKEMA
Sforzi-deformazione , Rilsan® MB 3610 NAT (Secco), PA11-I, ARKEMA
Modulo secante-deformazione , Rilsan® MB 3610 NAT (Secco), PA11-I, ARKEMA
Caratteristiche
Processabilità e Forma di Forni
Estrusione Profilati
Forma fisica disponibile
Pellet, Colore naturale
Additivi
Plastificante
Caratteristiche speciali
Alto urto o modificato all'urto, Stabilizzato o stabile alla luce, Estab. agli U.V. o per applicaz.in esterni, Stabilizzato o stabile al calore
Certifications
Contiene risorse rinnovabili
Disponibilità geografica
Altre informazioni
Altre Estrusioni

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 230°C / 250°C / 280°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-8 hours at 80-90°C.

Resistenza chimica
Acidi
Acido acetico (5% da massa) (23°C)
Soluzione acida citrica (10% da massa) (23°C)
Acido lattico (10% da massa) (23°C)
Acido cloridrico (36% da massa) (23°C)
Acido nitrico (40% da massa) (23°C)
Acido solforico (38% da massa) (23°C)
Acido solforico (5% da massa) (23°C)
Soluzione acida cromica (40% da massa) (23°C)
Basi
Soluzione dell' idrossido del sodio (35% da massa) (23°C)
Soluzione dell' idrossido del sodio (1% da massa) (23°C)
Soluzione dell' idrossido di ammonio (10% da massa) (23°C)
Alcool
Metanolo (23°C)
Etanolo (23°C)
Idrocarburi
n-Hexane (23°C)
Toluene (23°C)
Chetoni
Acetone (23°C)
Oli minerali
Olio multigrade del motore di SAE 10W40 (23°C)
Olio multigrade del motore di SAE 10W40 (130°C)
Olio dell' ipoide-ingranaggio di SAE 80/90 (130°C)
Olio isolante (23°C)
Combustibili Standard
Liquido 1 di ISO 1817 (60°C)
Liquido 2 di ISO 1817 (60°C)
Liquido 3 di ISO 1817 (60°C)
Liquido 4 di ISO 1817 (60°C)
Combust. stand. senza alcool (pref. ISO 1817 liquido C) (23°C)
Combust. stand. con alcool (pref. ISO 1817 liquido 4) (23°C)
Combustibile diesel (pref. ISO 1817 liquido F) (23°C)
Combustibile diesel (pref. ISO 1817 liquido F) (90°C)
Combustibile diesel (pref. ISO 1817 liquido F) (>90°C)
Soluzioni saline
Soluzione del cloruro di sodio (10% da massa) (23°C)
Soluzione dell' ipoclorito del sodio (10% da massa) (23°C)
Soluzione del cloruro dello zinco (50% da massa) (23°C)
Altri
Acetato etilico (23°C)
Perossido di idrogeno (23°C)
Liquido di freno del DOT N° 4 (130°C)
Glicol etilenico (50% da massa) in acqua (108°C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.