Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsan® TIEFLEX S452 NAT T6L - PA* - ARKEMA

Material Data Center offers the following functions for Rilsan® TIEFLEX S452 NAT T6L:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Rilsan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Rilsan® TIEFLEX S452 NAT T6L resin is a flexible tie layer alloy partially based on renewable resources. This grade is designed for multilayer automotive and trucks lines (tie layer for fuel line). In the case of direct contact with fuel, contact Arkema representative for recommendations.

Packaging:
This grade is delivered dried in sealed packaging (25kg bags) ready to be processed.

Shelf life:
Two years from the date of delivery. For any use above this limit, please refer to our technical services.
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 3.7 / * cm³/10min ISO 1133
Temperatura 235 / * °C -
Carico 5 / * kg -
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 685 / 515 MPa ISO 527
Carico unitario a trazione - / 33 MPa ISO 527
Deformazione a snervamento - / 31 % ISO 527
Deformazione nominale a rottura - / >50 % ISO 527
Resistenzia all'urto Charpy con intaglio, +23°C - / 95 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C - / 6.5 kJ/m² ISO 179/1eA
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 217 / * °C ISO 11357-1/-3
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 2.9 / * % Sim. alla ISO 62
Assorbimento d'umidità 1.2 / * % Sim. alla ISO 62
Massa volumica 1090 / - kg/m³ ISO 1183
Caratteristiche
Processabilità e Forma di Forni
Altre Estrusioni
Forma fisica disponibile
Pellet, Colore naturale
Certifications
Contiene risorse rinnovabili
Disponibilità geografica
Altre informazioni
Altre Estrusioni
Processing conditions
- Typical melt temperature (min / recommended / max): 220°C / 230°C / 270°C
- Drying time and temperature (only necessary for bags opened for more than two hours): 4-6 hours at 80°C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.