Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Sarlink® EE-2280B - TPS - Teknor Apex Co.

Material Data Center offers the following functions for Sarlink® EE-2280B:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Sarlink datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
For more detailed information, please read our brochure p. 46 to 54
or contact our representatives in your region.
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Deformazione residua dopo compressione a 23°C, 24h 31 % ISO 815
Deformazione residua dopo compressione a 70°C, 24h 49 % ISO 815
Durezza Shore A 83 - ISO 7619-1
Other Standards[S]
Carico Unitario al 100% di allungamento 3.8 MPa ISO 37
Carico Unitario a rottura TPE 8.1 MPa ISO 37
Allungamento a rottura TPE 610 % ISO 37
S: These properties are reported by the producer according standards that are different to our defaults.
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1180 kg/m³ ISO 1183
Caratteristiche
Processabilità e Forma di Forni
Altre Estrusioni
Caratteristiche speciali
Estab. agli U.V. o per applicaz.in esterni
Caratteristiche
Buona adesione
Resistenza Chimica
Resistenza all'ozono
Applicazioni
Automotive
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.