Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Solplast TH 30A9000 A - TPS - Uteksol d.o.o.

Material Data Center offers the following functions for Solplast TH 30A9000 A:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Solplast datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di Fluiditá, MFI 8 g/10min ISO 1133
Temperatura 190 °C -
Carico 5 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Resistenza a trazione 5.5 MPa ISO 37
Deformazione a rottura 960 % ISO 37
Deformazione residua dopo compressione a 23°C, 24h 11 % ISO 815
Deformazione residua dopo compressione a 70°C, 24h 27 % ISO 815
Deformazione residua dopo compressione a 100°C, 24h 47 % ISO 815
Resistenza alla lacerazione 14 kN/m ISO 34-1
Durezza Shore A 30 - ISO 7619-1
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1080 kg/m³ ISO 1183
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Temperatura di fusione 170 - 230 °C -
Temperatura dello stampo 30 - 40 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Colore naturale
Caratteristiche speciali
Estab. agli U.V. o per applicaz.in esterni
Caratteristiche
Copolimero
Disponibilità geografica
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.