Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of STYRON™ HIPS - (PS-HI) - Trinseo

Material Data Center offers the following functions for STYRON™ HIPS:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Styron datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di Fluiditá, MFI 6.3 g/10min ISO 1133
Temperatura 200 °C -
Carico 5 kg -
ASTM Data
Indice di fluidità a caldo, MFI 6.3 g/10min ASTM D 1238
Temperatura 200 °C -
Carico 5 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 2700 MPa ISO 527
Carico unitario a trazione 33 MPa ISO 527
Carico unitario a rottura 27 MPa ISO 527
Deformazione a rottura 20 % ISO 527
Modulo a flessione, 23°C 2600 MPa ISO 178
Resistenza alla flessione 62 MPa ISO 178
ASTM Data
Modulo a trazione 2700 MPa ASTM D 638
Resistenza alla trazione di snervamento 33 MPa ASTM D 638
Resistenza alla trazione a rottura 27 MPa ASTM D 638
Allungamento a rottura 20 % ASTM D 638
Modulo a flessione 2600 MPa ASTM D 790
Resistenza alla flessione 62 MPa ASTM D 790
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 72 °C ISO 75-1/-2
Temp.di rammollimento Vicat, A 100 °C ISO 306
ASTM Data
UL 94 combustibilitá HB - UL 94
Spessore testati 1.5 mm -
DTUL a 264 psi 72 °C ASTM D 648
Temp.di rammollimento Vicat 100 °C ASTM D 1525
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1050 kg/m³ ISO 1183
Densità 1050 kg/m³ ASTM D 792
Caratteristiche
Processabilità e Forma di Forni
Altre Estrusioni, Termoformatura
Caratteristiche speciali
Alto urto o modificato all'urto, Stabilizzato o stabile al calore, Trasparente
Caratteristiche
High Gloss
Certifications
Contatto con gli alimenti, Approvato per l'utilizzo per contatto con alimenti 10/2011, Approvato per l'utilizzo per contatto con alimenti secondo la FDA 21 CFR
Applicazioni
Imballaggio
Disponibilità geografica
Europa, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.