Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of TROGAMID® myCX - PAPACM12 - Evonik Operations GmbH

Material Data Center offers the following functions for TROGAMID® myCX:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Trogamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Microcrystalline, permanently transparent polyamide

TROGAMID® myCX is a microcrystalline transparent polyamide for the manufacture of parts in the optical industry, like lenses according the injection molding procedure. 

The crystallites are so small, that they do not scatter visible light, and the material appears transparent to the human eye.

The crystalline structure causes the excellent crack resistance for this polymer. TROGAMID® myCX is supplied as spherical pellets in polyethylene- packaging. Deviations of molds or in processing are possible to a certain extent, if they are required by the cavity or the process itself. 

Pigmentation may affect values.

For information about processing of TROGAMID®, please follow the general commendations about “Processing of TROGAMID® compounds”. 
 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.TROGAMID.COM

Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 8.2 / * cm³/10min ISO 1133
Temperatura 280 / * °C -
Carico 2.16 / * kg -
Ritiro di stampaggio, parallelo 0.7 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.7 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 1400 / - MPa ISO 527
Carico unitario a trazione 60 / - MPa ISO 527
Deformazione a snervamento 8 / - % ISO 527
Deformazione nominale a rottura >50 / - % ISO 527
Modulo di scorrimento a trazione, 1h * / 1300 MPa ISO 899-1
Modulo di scorrimento a trazione, 1000h * / 700 MPa ISO 899-1
Resistenza all'urto Charpy, +23°C N / - kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C N / - kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 16 / 11 kJ/m² ISO 179/1eA
Type of failure C / C - -
Resistenzia all'urto Charpy con intaglio, -30°C 14 / 10 kJ/m² ISO 179/1eA
Type of failure C / C - -
Durezza Shore D 81 / * - ISO 7619-1
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 255 / * °C ISO 11357-1/-3
Temperatura di transizione vetrosa, 10°C/min 140 / * °C ISO 11357-1/-2
Temp.di inflessione sotto carico, 1.80 MPa 105 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 122 / * °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 130 / * °C ISO 306
Coeff.di dilatazione termica lin., parallelo 90 / * E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 90 / * E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm HB / * class IEC 60695-11-10
Spessore provato 1.6 / * mm -
Reazione al fuoco a spessore h HB / * class IEC 60695-11-10
Spessore provato 0.8 / * mm -
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 3.6 / - - IEC 62631-2-1
Costante dielettrica relativa, 1MHz 3.2 / - - IEC 62631-2-1
Fattore di dissipazione, 100Hz 115 / - E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 325 / - E-4 IEC 62631-2-1
Resistività volumica >1E13 / - Ohm*m IEC 62631-3-1
Rigidità dielettrica 27 / - kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali 600 / - - IEC 60112
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 3.5 / * % Sim. alla ISO 62
Assorbimento d'umidità 1.5 / * % Sim. alla ISO 62
Massa volumica 1020 / - kg/m³ ISO 1183
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Estrusione Film, Estrusione Profilati
Forma fisica disponibile
Granuli
Caratteristiche speciali
Stabilizzato o stabile alla luce, Estab. agli U.V. o per applicaz.in esterni, Trasparente
Resistenza Chimica
Resistenza alla rottura da stress ambientale
Certifications
Contatto con gli alimenti, Grado medico, Approvazione della USP class VI
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.