Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultradur® B 4315 G6 HR - PBT-I-GF30 - BASF

Material Data Center offers the following functions for Ultradur® B 4315 G6 HR:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultradur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Injection-moulding grade containing 30% glass-fibres, for rigid,tough and dimensionally stable technical parts, used in applications with highest demands on hydrolysis resistance such es automotive connectors and housings for electronic units under the hood.
The black colored product Ultradur® B4315 G6 HR BK15045 has a LS coloration (Laser Sensitive) and can be marked with Nd:YAG lasers.

Abbreviated designation according to ISO 1043: PBT-I-GF30
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 15 cm³/10min ISO 1133
Temperatura 275 °C -
Carico 2.16 kg -
Ritiro di stampaggio, parallelo 0.5 % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 1.1 % ISO 294-4, 2577
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 9200 MPa ISO 527
Carico unitario a rottura 130 MPa ISO 527
Deformazione a rottura 3.2 % ISO 527
Resistenza all'urto Charpy, +23°C 75 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C 65 kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 10 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 8 kJ/m² ISO 179/1eA
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 223 °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 205 °C ISO 75-1/-2
Reaz. al fuoco spess.nom. 1.5mm HB class IEC 60695-11-10
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Res. Alle correnti striscianti superficiali 400 - IEC 60112
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1510 kg/m³ ISO 1183
Proprietà Specifiche MaterialeValoreUnitáNorma del test
ISO Data
Numero di viscosità 103 cm³/g ISO 307, 1157, 1628
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 80 - 120 °C -
Pre-essiccamento - Tempo 4 h -
Umidità del Processo ≤0.04 % -
Temperatura di fusione 250 - 280 °C -
Temperatura dello stampo 60 - 100 °C -
Funzioni
Sforzi-deformazione , Ultradur® B 4315 G6 HR, PBT-I-GF30, BASF
Modulo secante-deformazione , Ultradur® B 4315 G6 HR, PBT-I-GF30, BASF
Sforzi-deformazioni (isocrona) 23°C, Ultradur® B 4315 G6 HR, PBT-I-GF30, BASF
Modulo di scorrimento-tempo 23°C, Ultradur® B 4315 G6 HR, PBT-I-GF30, BASF
Curva di scorrimento 23°C, Ultradur® B 4315 G6 HR, PBT-I-GF30, BASF
Sforzi-deformazioni (isocrona) 40°C, Ultradur® B 4315 G6 HR, PBT-I-GF30, BASF
Modulo di scorrimento-tempo 40°C, Ultradur® B 4315 G6 HR, PBT-I-GF30, BASF
Curva di scorrimento 40°C, Ultradur® B 4315 G6 HR, PBT-I-GF30, BASF
Sforzi-deformazioni (isocrona) 90°C, Ultradur® B 4315 G6 HR, PBT-I-GF30, BASF
Modulo di scorrimento-tempo 90°C, Ultradur® B 4315 G6 HR, PBT-I-GF30, BASF
Curva di scorrimento 90°C, Ultradur® B 4315 G6 HR, PBT-I-GF30, BASF
Sforzi-deformazioni (isocrona) 120°C, Ultradur® B 4315 G6 HR, PBT-I-GF30, BASF
Modulo di scorrimento-tempo 120°C, Ultradur® B 4315 G6 HR, PBT-I-GF30, BASF
Curva di scorrimento 120°C, Ultradur® B 4315 G6 HR, PBT-I-GF30, BASF
Sforzi-deformazioni (isocrona) 160°C, Ultradur® B 4315 G6 HR, PBT-I-GF30, BASF
Modulo di scorrimento-tempo 160°C, Ultradur® B 4315 G6 HR, PBT-I-GF30, BASF
Curva di scorrimento 160°C, Ultradur® B 4315 G6 HR, PBT-I-GF30, BASF
Modulo a taglio-temperatura , Ultradur® B 4315 G6 HR, PBT-I-GF30, BASF
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Caratteristiche speciali
Alto urto o modificato all'urto
Resistenza Chimica
Stabilità idrolitica
Applicazioni
Automotive, Elettrotecnica ed electrici
Altre informazioni
Stampaggio ad Iniezione
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 250 - 280 °C
injection molding, Melt temperature, recommended: 260 °C
injection molding, Mold temperature, range: 60 - 100 °C
injection molding, Mold temperature, recommended: 80 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.