Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultraform® N2200 G53 Q600 - POM-GF25 - BASF

Material Data Center offers the following functions for Ultraform® N2200 G53 Q600:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultraform datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Injection molding grade for parts requiring high stiffness and strength together with good mold release.

Abbreviated designation according to ISO 1043-1: POM-GF25
Designation according to ISO 29988-POM-K,GF25,M-GNR,2-3
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 4 cm³/10min ISO 1133
Temperatura 190 °C -
Carico 2.16 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 8800 MPa ISO 527
Carico unitario a rottura 130 MPa ISO 527
Deformazione a rottura 3 % ISO 527
Modulo di scorrimento a trazione, 1h 7500 MPa ISO 899-1
Modulo di scorrimento a trazione, 1000h 5800 MPa ISO 899-1
Resistenza all'urto Charpy, +23°C 55 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C 60 kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 9 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 8.5 kJ/m² ISO 179/1eA
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 168 °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 163 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 165 °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 160 °C ISO 306
Coeff.di dilatazione termica lin., parallelo 35 E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm HB class IEC 60695-11-10
Spessore provato 1.6 mm -
Yellow Card disponibile - -
Reazione al fuoco a spessore h HB class IEC 60695-11-10
Spessore provato 0.8 mm -
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 4 - IEC 62631-2-1
Costante dielettrica relativa, 1MHz 4 - IEC 62631-2-1
Fattore di dissipazione, 100Hz 40 E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 70 E-4 IEC 62631-2-1
Resistività volumica 1E12 Ohm*m IEC 62631-3-1
Resistività superficiale 1E14 Ohm IEC 62631-3-2
Rigidità dielettrica 43 kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali 600 - IEC 60112
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'acqua 0.9 % Sim. alla ISO 62
Assorbimento d'umidità 0.15 % Sim. alla ISO 62
Massa volumica 1580 kg/m³ ISO 1183
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Temperatura di fusione 190 - 220 °C -
Temperatura dello stampo 80 - 110 °C -
Funzioni
Viscosità-Velocità di taglio , Ultraform® N2200 G53 Q600, POM-GF25, BASF
Sforzo di taglio-Velocità di taglio , Ultraform® N2200 G53 Q600, POM-GF25, BASF
Modulo dinamico a taglio-temperatura , Ultraform® N2200 G53 Q600, POM-GF25, BASF
Sforzi-deformazione , Ultraform® N2200 G53 Q600, POM-GF25, BASF
Modulo secante-deformazione , Ultraform® N2200 G53 Q600, POM-GF25, BASF
Sforzi-deformazioni (isocrona) 23°C, Ultraform® N2200 G53 Q600, POM-GF25, BASF
Modulo di scorrimento-tempo 23°C, Ultraform® N2200 G53 Q600, POM-GF25, BASF
Curva di scorrimento 23°C, Ultraform® N2200 G53 Q600, POM-GF25, BASF
Sforzi-deformazioni (isocrona) 40°C, Ultraform® N2200 G53 Q600, POM-GF25, BASF
Modulo di scorrimento-tempo 40°C, Ultraform® N2200 G53 Q600, POM-GF25, BASF
Curva di scorrimento 40°C, Ultraform® N2200 G53 Q600, POM-GF25, BASF
Sforzi-deformazioni (isocrona) 60°C, Ultraform® N2200 G53 Q600, POM-GF25, BASF
Modulo di scorrimento-tempo 60°C, Ultraform® N2200 G53 Q600, POM-GF25, BASF
Curva di scorrimento 60°C, Ultraform® N2200 G53 Q600, POM-GF25, BASF
Sforzi-deformazioni (isocrona) 80°C, Ultraform® N2200 G53 Q600, POM-GF25, BASF
Modulo di scorrimento-tempo 80°C, Ultraform® N2200 G53 Q600, POM-GF25, BASF
Curva di scorrimento 80°C, Ultraform® N2200 G53 Q600, POM-GF25, BASF
Sforzi-deformazioni (isocrona) 100°C, Ultraform® N2200 G53 Q600, POM-GF25, BASF
Modulo di scorrimento-tempo 100°C, Ultraform® N2200 G53 Q600, POM-GF25, BASF
Curva di scorrimento 100°C, Ultraform® N2200 G53 Q600, POM-GF25, BASF
Sforzi-deformazioni (isocrona) 120°C, Ultraform® N2200 G53 Q600, POM-GF25, BASF
Modulo di scorrimento-tempo 120°C, Ultraform® N2200 G53 Q600, POM-GF25, BASF
Curva di scorrimento 120°C, Ultraform® N2200 G53 Q600, POM-GF25, BASF
Volume specifico-temperatura (pvT) , Ultraform® N2200 G53 Q600, POM-GF25, BASF
Modulo a taglio-temperatura , Ultraform® N2200 G53 Q600, POM-GF25, BASF
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet
Additivi
Agente di distacco
Caratteristiche
Copolimero
Disponibilità geografica
Altre informazioni
Stampaggio ad Iniezione
PROCESSING
injection molding, Melt temperature, range: 190 - 220 °C
injection molding, Melt temperature, recommended: 200 °C
injection molding, Mold temperature, range: 80 - 110 °C
injection molding, Mold temperature, recommended: 90 °C
Resistenza chimica
Acidi
Acido acetico (5% da massa) (23°C)
Acido lattico (10% da massa) (23°C)
Acido cloridrico (36% da massa) (23°C)
Acido nitrico (40% da massa) (23°C)
Acido solforico (38% da massa) (23°C)
Acido solforico (5% da massa) (23°C)
Soluzione acida cromica (40% da massa) (23°C)
Basi
Soluzione dell' idrossido del sodio (35% da massa) (23°C)
Soluzione dell' idrossido del sodio (1% da massa) (23°C)
Soluzione dell' idrossido di ammonio (10% da massa) (23°C)
Alcool
Alcool di isopropile (23°C)
Metanolo (23°C)
Etanolo (23°C)
Idrocarburi
n-Hexane (23°C)
Toluene (23°C)
isoottano (23°C)
Chetoni
Acetone (23°C)
Eteri
Etere Etilico (23°C)
Oli minerali
Olio multigrade del motore di SAE 10W40 (130°C)
Olio dell' ipoide-ingranaggio di SAE 80/90 (130°C)
Combustibili Standard
Liquido 1 di ISO 1817 (60°C)
Liquido 2 di ISO 1817 (60°C)
Liquido 3 di ISO 1817 (60°C)
Liquido 4 di ISO 1817 (60°C)
Combust. stand. senza alcool (pref. ISO 1817 liquido C) (23°C)
Combust. stand. con alcool (pref. ISO 1817 liquido 4) (23°C)
Combustibile diesel (pref. ISO 1817 liquido F) (23°C)
Combustibile diesel (pref. ISO 1817 liquido F) (>90°C)
Soluzioni saline
Soluzione del cloruro di sodio (10% da massa) (23°C)
Soluzione dell' ipoclorito del sodio (10% da massa) (23°C)
Soluzione del carbonato di sodio (20% da massa) (23°C)
Soluzione del carbonato di sodio (2% da massa) (23°C)
Altri
Acetato etilico (23°C)
Perossido di idrogeno (23°C)
Liquido di freno del DOT N° 4 (130°C)
Glicol etilenico (50% da massa) in acqua (108°C)
acido oleico 50% + olio di oliva 50% (23°C)
Acqua (23°C)
Acqua deionizzata (90°C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.