Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrafuse PPSU - PPSU - BASF

Material Data Center offers the following functions for Ultrafuse PPSU:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrafuse datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 39 cm³/10min ISO 1133
Temperatura 360 °C -
Carico 10 kg -
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di transizione vetrosa, 10°C/min 220 °C ISO 11357-1/-2
Temp.di inflessione sotto carico, 1.80 MPa 212 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 218 °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 220 °C ISO 306
Coeff.di dilatazione termica lin., parallelo 55 E-6/K ISO 11359-1/-2
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1210 kg/m³ ISO 1183
3D DataValoreUnitáNorma del test
Other Standards[S]
Modulo a trazione, flat 2040 MPa ISO 527
Modulo a trazione, upright 2040 MPa ISO 527
Resistenza a trazione, flat 65.1 MPa ISO 527
Resistenza a trazione, upright 51.6 MPa ISO 527
Deformazione a rottura, flat 6.5 % ISO 527
Deformazione a rottura, upright 3.2 % ISO 527
Modulo a flessione, flat 2150 MPa ISO 178
Modulo a flessione, upright 2000 MPa ISO 178
Resistenza alla flessione, flat 92.6 MPa ISO 178
Resistenza alla flessione, upright 96.5 MPa ISO 178
Resistenza all'urto Charpy, +23°C, flat 201 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, +23°C, upright 22.6 kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C, flat 13.8 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, +23°C, upright 5.5 kJ/m² ISO 179/1eA
Resistenza all'urto Izod, +23°C, flat 119 kJ/m² ISO 180/1U
Resistenza all'urto Izod, +23°C, upright 14.3 kJ/m² ISO 180/1U
Resistenza all'urto Izod con intaglio, +23°C, flat 12 kJ/m² ISO 180/1A
Resistenza all'urto Izod con intaglio, +23°C, upright 5.5 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
Caratteristiche
Processabilità e Forma di Forni
Additive Manufacturing
Forma fisica disponibile
Monofilament
Caratteristiche
Buona adesione, Stabilità termica
Resistenza Chimica
Resistenza chimica generale
Disponibilità geografica
Nord America, Europa, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.