Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrafuse TPU 85A - TPU - BASF

Material Data Center offers the following functions for Ultrafuse TPU 85A:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrafuse datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 14.8 cm³/10min ISO 1133
Temperatura 190 °C -
Carico 3.8 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Deformazione residua dopo compressione a 70°C, 24h 52 % ISO 815
Resistenza all'abrasione 82 mm³ ISO 4649
Durezza Shore A 90 - ISO 7619-1
Durezza Shore D 37 - ISO 7619-1
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di transizione vetrosa, 10°C/min -44 °C ISO 11357-1/-2
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1080 kg/m³ ISO 1183
3D DataValoreUnitáNorma del test
Other Standards[S]
Modulo a trazione, flat 20 MPa ISO 527
Modulo a trazione, upright 27 MPa ISO 527
Carico unitario a rottura, flat 34 MPa ISO 527
Carico unitario a rottura, upright 10 MPa ISO 527
Deformazione a rottura, flat 600 % ISO 527
Deformazione a rottura, upright 320 % ISO 527
Resistenza all'urto Charpy, -30°C, flat 0 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C, on-edge 0 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C, upright 0 kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C, flat 0 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, +23°C, on-edge 0 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, +23°C, upright 0 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C, flat 47.3 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C, on-edge 95.4 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C, upright 9.3 kJ/m² ISO 179/1eA
Resistenza all'urto Izod con intaglio, +23°C, flat 0 kJ/m² ISO 180/1A
Resistenza all'urto Izod con intaglio, +23°C, on-edge 0 kJ/m² ISO 180/1A
Resistenza all'urto Izod con intaglio, +23°C, upright 0 kJ/m² ISO 180/1A
Carico Unitario al 50% di allungamento, flat 7.2 MPa ISO 527
Carico Unitario al 50% di allungamento, upright 6.2 MPa ISO 527
Carico Unitario al 100% di allungamento, flat 8.7 MPa ISO 527
Carico Unitario al 100% di allungamento, upright 7.5 MPa ISO 527
Carico Unitario al 200% di allungamento, flat 12.1 MPa ISO 527
Resistività volumica, flat 2.6E9 Ohm*m IEC 62631-3-1
Resistività volumica, on-edge 2.1E9 Ohm*m IEC 62631-3-1
Resistività volumica, upright 2.1E9 Ohm*m IEC 62631-3-1
S: These properties are reported by the producer according standards that are different to our defaults.
Caratteristiche
Processabilità e Forma di Forni
Additive Manufacturing
Forma fisica disponibile
Monofilament, Colore naturale, Bianco
Disponibilità geografica
Nord America, Europa, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com