Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrafuse Z PCTG - Copolyester-Z - BASF

Material Data Center offers the following functions for Ultrafuse Z PCTG:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrafuse datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 67.5 cm³/10min ISO 1133
Temperatura 275 °C -
Carico 5 kg -
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di transizione vetrosa, 10°C/min 81 °C ISO 11357-1/-2
Temp.di inflessione sotto carico, 1.80 MPa 69 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 73 °C ISO 75-1/-2
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1200 kg/m³ ISO 1183
3D DataValoreUnitáNorma del test
Other Standards[S]
Modulo a trazione, flat 1760 MPa ISO 527
Modulo a trazione, upright 1670 MPa ISO 527
Resistenza a trazione, flat 37.1 MPa ISO 527
Resistenza a trazione, upright 13.6 MPa ISO 527
Deformazione a rottura, flat 3.1 % ISO 527
Deformazione a rottura, upright 0.8 % ISO 527
Modulo a flessione, flat 1610 MPa ISO 178
Modulo a flessione, on-edge 1780 MPa ISO 178
Modulo a flessione, upright 1490 MPa ISO 178
Resistenza alla flessione, flat 55.5 MPa ISO 178
Resistenza alla flessione, on-edge 70.8 MPa ISO 178
Resistenza alla flessione, upright 20.2 MPa ISO 178
Resistenza all'urto Charpy, +23°C, on-edge 9.5 kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C, flat 2.1 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, +23°C, on-edge 2.6 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, +23°C, upright 0.9 kJ/m² ISO 179/1eA
Resistenza all'urto Izod, +23°C, flat 14.3 kJ/m² ISO 180/1U
Resistenza all'urto Izod, +23°C, on-edge 24.2 kJ/m² ISO 180/1U
Resistenza all'urto Izod, +23°C, upright 3.4 kJ/m² ISO 180/1U
Resistenza all'urto Izod con intaglio, +23°C, on-edge 3.4 kJ/m² ISO 180/1A
Resistività volumica, flat 40000 Ohm*m IEC 62631-3-1
Resistività volumica, on-edge 130 Ohm*m IEC 62631-3-1
S: These properties are reported by the producer according standards that are different to our defaults.
Caratteristiche
Processabilità e Forma di Forni
Additive Manufacturing
Forma fisica disponibile
Monofilament, Nero
Caratteristiche
Amorfo
Applicazioni
Elettrotecnica ed electrici
Disponibilità geografica
Nord America, Europa, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.