Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® B3ZG7 OSI BK23273 - PA6-GF35 - BASF

Material Data Center offers the following functions for Ultramid® B3ZG7 OSI BK23273:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultramid B datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Ultramid® B3ZG7 OSI BK2373 is a 35% glass reinforced, pigmented black, heat stabilized, impact modified Polyamide 6 injection molding grade. It was developed to meet demanding mechanical and chemical requirements for the automotive oil pan application.
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Ritiro di stampaggio, parallelo 0.2 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.6 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 10000 / 6170 MPa ISO 527
Carico unitario a rottura 170 / 112 MPa ISO 527
Deformazione a rottura 3.5 / 11 % ISO 527
Modulo a flessione, 23°C 8920 / 5650 MPa ISO 178
Resistenza all'urto Charpy, +23°C 102 / 106 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C 113 / - kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 26 / 34 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 18 / - kJ/m² ISO 179/1eA
Resistenza all'urto Izod con intaglio, +23°C 24 / 34 kJ/m² ISO 180/1A
Resistenza all'urto Izod con intaglio 17 / - kJ/m² ISO 180/1A
Temperatura -40 °C -
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 220 / * °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 206 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 220 / * °C ISO 75-1/-2
Coeff.di dilatazione termica lin., parallelo 13.1 / * E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 110 / * E-6/K ISO 11359-1/-2
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'umidità 1.7 / * % Sim. alla ISO 62
Massa volumica 1380 / - kg/m³ ISO 1183
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 80 °C -
Pre-essiccamento - Tempo 2 - 4 h -
Umidità del Processo ≤0.08 % -
Temperatura di fusione 270 - 295 °C -
Temperatura dello stampo 80 - 95 °C -
Zona 1 245 - 275 °C -
Zona 2 260 - 285 °C -
Zona 3 270 - 295 °C -
Temperatura dell ugello 270 - 295 °C -
Pressione di Iniezione 3.5 - 12.5 MPa -
Funzioni
Modulo dinamico a taglio-temperatura , Ultramid® B3ZG7 OSI BK23273 (Secco), PA6-GF35, BASF
Sforzi-deformazione , Ultramid® B3ZG7 OSI BK23273 (Secco), PA6-GF35, BASF
Sforzi-deformazione , Ultramid® B3ZG7 OSI BK23273 (cond.), PA6-GF35, BASF
Modulo secante-deformazione , Ultramid® B3ZG7 OSI BK23273 (Secco), PA6-GF35, BASF
Modulo secante-deformazione , Ultramid® B3ZG7 OSI BK23273 (cond.), PA6-GF35, BASF
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet, Nero
Caratteristiche speciali
Alto urto o modificato all'urto, Stabilizzato o stabile al calore
Resistenza Chimica
Resistenza all’olio
Applicazioni
Automotive
Disponibilità geografica
Nord America, Europa
Altre informazioni
Stampaggio ad Iniezione
PREPROCESSING
Pre/Post-processing, max. allowed water content: .08 %
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 2 - 4 h

PROCESSING
injection molding, Melt temperature, range: 270 - 295 °C
injection molding, Mold temperature, range: 80 - 95 °C

Material Handling
Max. Water content: 0.08%
Product is supplied in sealed containers and drying prior to molding is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 80 °C (176 °F) is recommended. Drying time is dependent on moisture level but 2-4 hours is generally sufficient.
Further information concerning safe handling procedures can be obtained from the Material Safety Data Sheet. Alternatively, please contact your BASF representative.

Typical Profile
Melt Temperature 270-295 °C (518-563 °F)
Mold Temperature 80-95 °C (176-203 °F)
Injection and Packing Pressure 35-125 bar (500-1800psi)
Rear Zone 245-275 °C (473-527 °F)
Center Zone 260-285 °C (500-545 °C)
Front Zone 270-295 °C (518-563 °F)
Nozzle 270-295 °C (518-563 °F)

Mold Temperatures
This product can be processed over a wide range of mold temperatures; however, for applications where aesthetics are critical, a mold surface temperature of 80-95 °C (176-203 °F) is required.

Pressures
Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off.

Back pressure can be utilized to provide uniform melt consistency and reduce trapped air and gas. Minimal back pressure should be utilized to prevent glass breakage. recommended to minimize glass fiber breakage.

Fill Rate
Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing. Surface appearance is directly affected by injection rate.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com