Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrasint PA11 ESD - PA11 - BASF

Material Data Center offers the following functions for Ultrasint PA11 ESD:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrasint datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 20 / * cm³/10min ISO 1133
Temperatura 220 / * °C -
Carico 2.16 / * kg -
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 204 / * °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 111 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 186 / * °C ISO 75-1/-2
Temp.di rammollimento Vicat, A 192 / * °C ISO 306
Temp.di rammollimento Vicat, B 183 / * °C ISO 306
Altre Proprietàsecco/condUnitáNorma del test
Massa volumica 1070 / - kg/m³ ISO 1183
Bulk density 460 kg/m³ -
3D Datasecco/condUnitáNorma del test
Other Standards[S]
Modulo a trazione, flat 3150 / 2300 MPa ISO 527
Modulo a trazione, upright 2150 / 1550 MPa ISO 527
Resistenza a trazione, flat 65 / 55 MPa ISO 527
Resistenza a trazione, upright 55 / 47 MPa ISO 527
Deformazione a rottura, flat 20 / 22 % ISO 527
Deformazione a rottura, upright 23 / 31 % ISO 527
Modulo a flessione, flat 3050 / 2550 MPa ISO 178
Modulo a flessione, upright 2100 / 1650 MPa ISO 178
Resistenza all'urto Charpy, +23°C, flat 80 / 101 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, +23°C, upright 90 / 107 kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C, flat 6.6 / 7.3 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, +23°C, upright 4.7 / 5.3 kJ/m² ISO 179/1eA
Resistenza all'urto Izod, +23°C, flat 67 / 81 kJ/m² ISO 180/1U
Resistenza all'urto Izod, +23°C, upright 58 / 83 kJ/m² ISO 180/1U
Resistenza all'urto Izod con intaglio, +23°C, flat 7 / 7.9 kJ/m² ISO 180/1A
Resistenza all'urto Izod con intaglio, +23°C, upright 5 / 5.5 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
Caratteristiche
Processabilità e Forma di Forni
Additive Manufacturing, Sinterizzazione a laser
Forma fisica disponibile
Polveri
Resistenza Chimica
Resistenza chimica generale
Certifications
Contiene risorse rinnovabili
Applicazioni
Elettrotecnica ed electrici
Disponibilità geografica
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.