Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrason® E 3010 NAT - PESU - BASF

Material Data Center offers the following functions for Ultrason® E 3010 NAT:
unit conversion, PDF datasheet print, comparison with other plastics, parameters for material models, CAE Interfaces

Check here, which other Ultrason E datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Unreinforced, higher viscosity injection moulding and extrusion grade, tougher and with improved chemical resistance.
Abbreviated designation according to ISO 1043-1: PESU
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 35 / * cm³/10min ISO 1133
Temperatura 360 / * °C -
Carico 10 / * kg -
Ritiro di stampaggio, parallelo 0.8 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.9 / * % ISO 294-4, 2577
ASTM Data
Ritiro di stampaggio, parallelo 0.007 mm/mm ASTM D 955
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione - / 2650 MPa ISO 527
Carico unitario a trazione - / 85 MPa ISO 527
Deformazione a snervamento - / 6.9 % ISO 527
Modulo di scorrimento a trazione, 1h * / 2800 MPa ISO 899-1
Resistenza all'urto Charpy, +23°C - / N kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C - / N kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C - / 8 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C * / 8 kJ/m² ISO 179/1eA
ASTM Data
Modulo a flessione 2599 / - MPa ASTM D 790
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di transizione vetrosa, 10°C/min 228 / * °C ISO 11357-1/-2
Temp.di inflessione sotto carico, 1.80 MPa 207 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 218 / * °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 215 / * °C ISO 306
Coeff.di dilatazione termica lin., parallelo 52 / * E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm V-0 / * class IEC 60695-11-10
Spessore provato 1.5 / * mm -
Yellow Card disponibile sì / * - -
Reazione al fuoco a spessore h V-0 / * class IEC 60695-11-10
Spessore provato 3.0 / * mm -
Yellow Card disponibile sì / * - -
Reazione al fuoco 5V a spess. h 5VA / * class IEC 60695-11-20
Spessore provato 3.0 / * mm -
Yellow Card disponibile sì / * - -
Indice di ossigeno 42.5 / * % ISO 4589-1/-2
ASTM Data
Temperatura di fusione 225 °C ASTM D 3418
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz * / 3.9 - IEC 62631-2-1
Costante dielettrica relativa, 1MHz * / 3.8 - IEC 62631-2-1
Fattore di dissipazione, 100Hz * / 17 E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz * / 140 E-4 IEC 62631-2-1
Resistività volumica * / >1E13 Ohm*m IEC 62631-3-1
Resistività superficiale * / >1E15 Ohm IEC 62631-3-2
Rigidità dielettrica * / 34 kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali * / 125 - IEC 60112
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 2.2 / * % Sim. alla ISO 62
Assorbimento d'umidità 0.8 / * % Sim. alla ISO 62
Massa volumica 1370 / - kg/m³ ISO 1183
Densità 1370 kg/m³ ASTM D 792
Proprietà Specifiche Materialesecco/condUnitáNorma del test
ISO Data
Numero di viscosità 66 / * cm³/g ISO 307, 1157, 1628
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 140 °C -
Pre-essiccamento - Tempo 4 h -
Umidità del Processo ≤0.02 % -
Temperatura di fusione 350 - 390 °C -
Temperatura dello stampo 140 - 180 °C -
Funzioni
Viscosità-Velocità di taglio , Ultrason® E 3010 NAT, PESU, BASF
Sforzo di taglio-Velocità di taglio , Ultrason® E 3010 NAT, PESU, BASF
Modulo dinamico a taglio-temperatura , Ultrason® E 3010 NAT (Secco), PESU, BASF
Sforzi-deformazione , Ultrason® E 3010 NAT (cond.), PESU, BASF
Modulo secante-deformazione , Ultrason® E 3010 NAT (cond.), PESU, BASF
Sforzi-deformazioni (isocrona) 23°C, Ultrason® E 3010 NAT (cond.), PESU, BASF
Modulo di scorrimento-tempo 23°C, Ultrason® E 3010 NAT (cond.), PESU, BASF
Curva di scorrimento 23°C, Ultrason® E 3010 NAT (cond.), PESU, BASF
Sforzi-deformazioni (isocrona) 140°C, Ultrason® E 3010 NAT (Secco), PESU, BASF
Modulo di scorrimento-tempo 140°C, Ultrason® E 3010 NAT (Secco), PESU, BASF
Curva di scorrimento 140°C, Ultrason® E 3010 NAT (Secco), PESU, BASF
Sforzi-deformazioni (isocrona) 180°C, Ultrason® E 3010 NAT (Secco), PESU, BASF
Modulo di scorrimento-tempo 180°C, Ultrason® E 3010 NAT (Secco), PESU, BASF
Curva di scorrimento 180°C, Ultrason® E 3010 NAT (Secco), PESU, BASF
Volume specifico-temperatura (pvT) , Ultrason® E 3010 NAT, PESU, BASF
Modulo a taglio-temperatura , Ultrason® E 3010 NAT (cond.), PESU, BASF
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Estrusione Film, Estrusione Profilati, Estrusione di Lastre/Fogli, Soffiaggio, Termoformatura
Forma fisica disponibile
Pellet, Colore naturale
Disponibilità geografica
Altre informazioni
Stampaggio ad Iniezione
PREPROCESSING
Pre/Post-processing, max. allowed water content: .02 %
Pre/Post-processing, Pre-drying, Temperature: 140 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 350 - 390 °C
injection molding, Melt temperature, recommended: 370 °C
injection molding, Mold temperature, range: 140 - 180 °C
injection molding, Mold temperature, recommended: 160 °C
injection molding, Dwell time, thermoplastics: 10 min

Pretreatment
Drying temperature: 130 - 150°C
Drying time: minimum 4h
recommended dryer: vaccum or dry air dryer
maximum moisture: 0,02 - 0,05%

Ultrason® can be injection molded by any type of machinery on the market, provided that the plasticizing unit and the mold temperature control system have been configured appropriately. The machinery manufacturer must be consulted if any doubts exist on the ability of various parts to withstand the high temperatures required (e.g. barrel, barrel head, bolted connections, etc.)

Long residence time in combination with high temperatures should be avoided e.g. by pump out material at regular intervals.
During extended interruptions, the barrel temperature should be lowered to about 250-280°C.

It has been found out that heating to the requested processing temperature and shutting down or lowering the temperature is best carried out in two steps.
First, the barrel temperatures are set at the lower processing temperature range for the particular thermoplastic (340 - 350 °C). As soon as these temperatures have reached a steady state, the material in the barrel is pumped out. Second, the barrel temperature can be set to the required processing temperature or the heaters can be shut down.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com