Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Utec® 4041 - (PE-UHMW) - Braskem

Material Data Center offers the following functions for Utec® 4041:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Utec datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Carico unitario a trazione 17 MPa ISO 527
Carico unitario a rottura 30 MPa ISO 527
Deformazione a rottura 400 % ISO 527
Resistenza all'urto Charpy, +23°C 120 kJ/m² ISO 179/1eU
Durezza Shore D 64 - ISO 7619-1
ASTM Data
Resistenza alla trazione di snervamento 17 MPa ASTM D 638
Resistenza alla trazione a rottura 30 MPa ASTM D 638
Allungamento a rottura 350 % ASTM D 638
Durezza D Shore 64 - ASTM D 2240
Resistenza all'urto Izod con intaglio, 1/8 in N J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di rammollimento Vicat, A 128 °C ISO 306
ASTM Data
coefficiente d’espansione termica, lung. 150 E-6/K ASTM D 696
DTUL a 66 psi 79 °C ASTM D 648
DTUL a 264 psi 48 °C ASTM D 648
Temperatura di fusione 133 °C ASTM D 3418
Temp.di rammollimento Vicat 128 °C ASTM D 1525
Conduttività termica, stato solido 0.0577 W/(m K) ASTM C 177
Proprietà ElettricheValoreUnitáNorma del test
ASTM Data
Rigidità elettrica, breve periodo di tempo 90 kV/mm ASTM D 149
Resistenza superficiale 1E12 Ohm ASTM D 257
Resistenza di volume 1E14 Ohm*cm ASTM D 257
Altre ProprietàValoreUnitáNorma del test
Assorbimento d’acqua, 24hr 0.01 % ASTM D 570
Densità 925 kg/m³ ASTM D 792
Viscosità intrinseca 18 dl/g -
Bulk Density 450 kg/m³ -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio a compressione
Caratteristiche speciali
Alto urto o modificato all'urto
Caratteristiche
Grado tribologico
Disponibilità geografica
Nord America, Europa, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.