Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® Care M40 R - PEEK - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® Care M40 R:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
High viscosity, unreinforced polyether ether ketone designed for the medical device industry
VESTAKEEP® Care is the ideal materials for the fabrication of medical devices with short time contact to human blood, tissue or bone for up to 30 days. VESTAKEEP® Care Grades have a good biocompatibility, processability and the option to pigment.

VESTAKEEP® Care M40 R are semi finished goods based on the high viscosity VESTAKEEP® Care M40 G polymer resin. 

The semi-crystalline polymer features superior thermal and chemical resistance.

Biocompatibility of VESTAKEEP® Care
In an extensive testing program run by independent certified labs, biocompatibility has been tested following United States Pharmacopeia and ISO 10933-1:2003 guidelines.
The test reports attest VESTAKEEP® Care’s excellent biocompatibility.

Biocompatibility tests for VESTAKEEP® Care:

 
Delivery of VESTAKEEP® Care
VESTAKEEP® Care M40 R rods can be produced in various diameters ranging from 6 mm up to 100 mm. The standard length is 1 m. Other dimensions are also available upon request.

Mechanical properties are evaluated on stock shapes test bars and further values are evaluated on injection molded samples.
The results shown have been generated from a low number of production lots. Therefore, they are preliminary and not yet the result of a statistical evaluation. Therefore they must not be used to establish specifications.


FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 11 cm³/10min ISO 1133
Temperatura 380 °C -
Carico 5 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 4050 MPa ISO 527
Carico unitario a trazione 110 MPa ISO 527
Deformazione a snervamento 5 % ISO 527
Deformazione nominale a rottura 40 % ISO 527
Durezza Shore D 84 - ISO 7619-1
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 155 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 205 °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 305 °C ISO 306
Coeff.di dilatazione termica lin., parallelo 60 E-6/K ISO 11359-1/-2
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Costante dielettrica relativa, 1MHz 2.8 - IEC 62631-2-1
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'acqua 0.5 % Sim. alla ISO 62
Massa volumica 1300 kg/m³ ISO 1183
Caratteristiche
Forma fisica disponibile
Prodotto semilavorato
Caratteristiche
Stabilità termica
Resistenza Chimica
Resistenza chimica generale
Certifications
Grado medico, Biocompatibility ISO 10993, Approvazione della USP class VI
Applicazioni
Medicale
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.