Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® 4000 CF30 - PEEK-CF30 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® 4000 CF30:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Carbon fiber-reinforced (30%), high viscosity polyether ether ketone

VESTAKEEP® 4000 CF30 is a carbon fiber reinforced (30%) polyether ether ketone for injection molding.

The semi-crystalline polymer features superior mechanical, thermal, and chemical resistance. Parts made from VESTAKEEP® 4000 CF30 are of low flammability.

VESTAKEEP® 4000 CF30 can be processed by common injection molding machines for thermoplastics.

We recommend a melt temperature between 380°C and 400°C during the injection molding process. The mold temperature should be within a range of 160°C to 200°C, preferably 180°C.

VESTAKEEP® 4000 CF30 is supplied as granules in 25 kg boxes with moisture-proof polyethylene liners.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

Pigmentation may affect values.

For information about processing VESTAKEEP® 4000 CF30, please follow the general recommendations in our brochure “VESTAKEEP® PEEK Processing Guidelines.“

The values presented are typical or average values, they do not constitute a specification. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT WWW.INDUSTRIAL.VESTAKEEP.COM
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 20 cm³/10min ISO 1133
Temperatura 380 °C -
Carico 21.6 kg -
Ritiro di stampaggio, parallelo 0 % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.4 % ISO 294-4, 2577
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 23000 MPa ISO 527
Carico unitario a rottura 240 MPa ISO 527
Deformazione a rottura 2 % ISO 527
Resistenza all'urto Charpy, +23°C 60 kJ/m² ISO 179/1eU
Type of failure C - -
Resistenza all'urto Charpy, -30°C 60 kJ/m² ISO 179/1eU
Type of failure C - -
Resistenzia all'urto Charpy con intaglio, +23°C 10 kJ/m² ISO 179/1eA
Type of failure C - -
Resistenzia all'urto Charpy con intaglio, -30°C 9 kJ/m² ISO 179/1eA
Type of failure C - -
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 340 °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 325 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 335 °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 340 °C ISO 306
Coeff.di dilatazione termica lin., parallelo 10 E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm V-0 class IEC 60695-11-10
Spessore provato 1.6 mm -
Reazione al fuoco a spessore h V-0 class IEC 60695-11-10
Spessore provato 0.8 mm -
Indice di ossigeno 47 % ISO 4589-1/-2
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Costante dielettrica relativa, 1MHz 17 - IEC 62631-2-1
Fattore di dissipazione, 1MHz 230 E-4 IEC 62631-2-1
Resistività volumica 10000 Ohm*m IEC 62631-3-1
Resistività superficiale 1000000 Ohm IEC 62631-3-2
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'acqua 0.4 % Sim. alla ISO 62
Massa volumica 1400 kg/m³ ISO 1183
Preparazione ProvetteValoreUnitáNorma del test
ISO Data
Stamp. ad Iniezione, temp. di fusione 420 °C ISO 294
Stamp. ad Iniezione, temperatura dello stampo 200 °C ISO 294
Stamp. ad Iniezione, velocità media d'iniezione 200 mm/s ISO 294
Stamp. ad Iniezione, pressione di chiusura 120 MPa ISO 294
Funzioni
Modulo a taglio-temperatura , VESTAKEEP® 4000 CF30, PEEK-CF30, Evonik
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Altre Estrusioni
Forma fisica disponibile
Pellet
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.