Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® i5 R - PEEK - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® i5 R:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Implantable grade polyether ether ketone rod stock for permanent implants

VESTAKEEP® i5 R is rod stock based on implantable grade neat polyether ether ketone resin VESTAKEEP® i5 G.

Proven Biocompatibility of VESTAKEEP® i-Grades

The extra high purity and extended quality measures make VESTAKEEP® i-grade materials an excellent choice for permanent implants.

The biocompatibility of VESTAKEEP® i5 R has been tested following ISO 10993-1 recommendations for permanent tissue/bone contact and USP Class VI.

VESTAKEEP® i5 R complies to ASTM F2026 “Standard Specification for Polyetheretherketone (PEEK) Polymers for Surgical Implant Applications”.
 
A summary of biocompatibility test results is available upon request.

Biocompatibility tests available for i5 R



Delivery of VESTAKEEP® i-Grades
VESTAKEEP® i5 R rods are available in different diameters and lengths.

Dimensions of VESTAKEEP® i5 R
Diameter Standard length*
6 to 20 mm 3000 mm
25 to 60 mm 2000 mm
70 to 100 mm 1000 mm
* Custom lengths are also available

The values presented are typical or average values, they do not constitute a specification. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY


 
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 3900 MPa ISO 527
Carico unitario a trazione 105 MPa ISO 527
Deformazione a snervamento 4.6 % ISO 527
Deformazione nominale a rottura 20 % ISO 527
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 340 °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 155 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 205 °C ISO 75-1/-2
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Costante dielettrica relativa, 1MHz 2.8 - IEC 62631-2-1
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'acqua 0.4 % Sim. alla ISO 62
Assorbimento d'umidità 0.12 % Sim. alla ISO 62
Massa volumica 1300 kg/m³ ISO 1183
Caratteristiche
Forma fisica disponibile
Prodotto semilavorato
Certifications
Grado medico, Biocompatibility ISO 10993, Approvazione della USP class VI
Applicazioni
Medicale
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com