Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® DX9303 BK E70288 - PA612-I - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® DX9303 BK E70288:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
High-viscosity, plasticized, heat- and light-stabilized, impact-modified polyamide 612 compound for extrusion

VESTAMID® DX9303 BK E70288 is a PA 612 extrusion compound developed for the production of tubing systems with higher requirements for heat resistance.

The melting point of VESTAMID® DX9303 BK E70288 is about 35°C higher than PA 11 and PA 12 compounds, allows higher peak temperatures in use. Thereby this compound fulfills the increased demands resulting from higher temperatures in the engine compartment.

If it is intended to use VESTAMID® DX9303 BK E70288 for fuel lines, certain preconditions must be observed. The Technical Marketing assists you in finding the suitable VESTAMID® compound.
At temperatures above 100°C tubing of VESTAMID® DX9303 BK E70288 allow a higher pressure load than tubing made of PA 12 compounds with comparable flexibility.

The process temperatures should be in the range of 240-270°C.

The material absorbs only little moisture. Therefore dimensions and properties of parts are nearly unaffected through ambient conditions.


Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general recommendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 11 / * cm³/10min ISO 1133
Temperatura 275 / * °C -
Carico 5 / * kg -
Ritiro di stampaggio, parallelo 2.7 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.9 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 900 / 680 MPa ISO 527
Carico unitario a trazione 38 / - MPa ISO 527
Deformazione a snervamento 30 / - % ISO 527
Deformazione nominale a rottura >50 / - % ISO 527
Resistenza all'urto Charpy, +23°C N / N kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C N / N kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 87 / 135 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 11 / 15 kJ/m² ISO 179/1eA
Type of failure C / C(P)[C(P)] - -
Durezza Shore D 70 / * - ISO 7619-1
C(P): CAMPUS
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 211 / * °C ISO 11357-1/-3
Temperatura di transizione vetrosa, 10°C/min 20 / * °C ISO 11357-1/-2
Temp.di inflessione sotto carico, 1.80 MPa 60 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 142 / * °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 159 / * °C ISO 306
Coeff.di dilatazione termica lin., parallelo 150 / * E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 120 / * E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm HB / * class IEC 60695-11-10
Spessore provato 1.6 / * mm -
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 4.7 / - - IEC 62631-2-1
Costante dielettrica relativa, 1MHz 2.7 / - - IEC 62631-2-1
Fattore di dissipazione, 100Hz 1450 / - E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 400 / - E-4 IEC 62631-2-1
Resistività volumica 2E10 / 5.3E8 Ohm*m IEC 62631-3-1
Rigidità dielettrica 39 / 34 kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali 600 / - - IEC 60112
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 2.4 / * % Sim. alla ISO 62
Assorbimento d'umidità 1 / * % Sim. alla ISO 62
Massa volumica 1050 / - kg/m³ ISO 1183
Preparazione ProvetteValoreUnitáNorma del test
ISO Data
Stamp. ad Iniezione, temp. di fusione 250 °C ISO 294
Stamp. ad Iniezione, temperatura dello stampo 80 °C ISO 294
Stamp. ad Iniezione, velocità media d'iniezione 200 mm/s ISO 294
Caratteristiche
Processabilità e Forma di Forni
Estrusione di tubi, Altre Estrusioni
Forma fisica disponibile
Pellet, Nero
Additivi
Plastificante
Caratteristiche speciali
Alto urto o modificato all'urto, Stabilizzato o stabile alla luce, Stabilizzato o stabile al calore
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.