Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® L1930 BK 9.7503 - PA12-GD30 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® L1930 BK 9.7503:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Glass fiber-reinforced, heat stabilized polyamide 12 compound

VESTAMID® L1930 BK 9.7503 is a heat stabilized, with 30% milled glass fiber-reinforced PA 12 compound suitable for injection molding.

Due to the reinforcement moldings from this compound exhibit a high strength and rigidity. Because PA 12 absorbs only little water, the parts have a good dimensional stability and almost unaffected mechanical properties at changing ambient humidity.

Due to the reinforcement the shrinking of moldings is decreased compared with unreinforced compounds. Using specialty short glass fibers for the reinforcement of VESTAMID® L1930 BK 9.7503 the difference between longitudinal and transverse shrinkage relating to the flow direction of the melt is significantly lower than with common glass fiber-reinforced products. Therefore especially low-warpage precision parts can be molded.

As a semi-crystalline material VESTAMID® L1930 BK 9.7503 feature an outstanding chemical resistance, e.g., against fuels, oils and fats.

VESTAMID® L1930 BK 9.7503 is supplied as cylindrical pellets in moisture-proof packaging.

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 27 / * cm³/10min ISO 1133
Temperatura 250 / * °C -
Carico 5 / * kg -
Ritiro di stampaggio, parallelo 0.5 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.5 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 3800 / 2970 MPa ISO 527
Carico unitario a trazione 65 / 58 MPa ISO 527
Deformazione a snervamento 5 / 8 % ISO 527
Deformazione nominale a rottura 11 / 15 % ISO 527
Resistenza all'urto Charpy, +23°C 75 / 82 kJ/m² ISO 179/1eU
Type of failure C / C - -
Resistenza all'urto Charpy, -30°C 65 / 72 kJ/m² ISO 179/1eU
Type of failure C / C - -
Resistenzia all'urto Charpy con intaglio, +23°C 7 / 6 kJ/m² ISO 179/1eA
Type of failure C / C - -
Resistenzia all'urto Charpy con intaglio, -30°C 6 / 5 kJ/m² ISO 179/1eA
Type of failure C / C - -
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 177 / * °C ISO 11357-1/-3
Temperatura di transizione vetrosa, 10°C/min 44 / * °C ISO 11357-1/-2
Temp.di inflessione sotto carico, 1.80 MPa 130 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 170 / * °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 170 / * °C ISO 306
Reaz. al fuoco spess.nom. 1.5mm HB / * class IEC 60695-11-10
Spessore provato 1.6 / * mm -
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 4.2 / 5.3 - IEC 62631-2-1
Costante dielettrica relativa, 1MHz 3.5 / 3.5 - IEC 62631-2-1
Fattore di dissipazione, 100Hz 360 / 860 E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 340 / 460 E-4 IEC 62631-2-1
Resistività volumica 1E13 / 1.5E12 Ohm*m IEC 62631-3-1
Rigidità dielettrica 48 / 45 kV/mm IEC 60243-1
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 1.1 / * % Sim. alla ISO 62
Assorbimento d'umidità 0.5 / * % Sim. alla ISO 62
Massa volumica 1240 / - kg/m³ ISO 1183
Preparazione ProvetteValoreUnitáNorma del test
ISO Data
Stamp. ad Iniezione, temp. di fusione 250 °C ISO 294
Stamp. ad Iniezione, temperatura dello stampo 80 °C ISO 294
Stamp. ad Iniezione, velocità media d'iniezione 200 mm/s ISO 294
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet, Nero
Caratteristiche speciali
Stabilizzato o stabile al calore
Caratteristiche
Bassa deformazione
Resistenza Chimica
Resistenza chimica generale, Resistenza al grasso, Resistenza all’olio
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.