Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® L2141 BK 9.7504 - PA12 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® L2141 BK 9.7504:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto

High viscosity PA12-Plastic resin for the extrusion

VESTAMID® L2141 BK 9.7504 is a heatstabilized polyamide 12 compound for the extrusion of tubing (e.g. fuel lines) and semi-finished products. Tubing according to DIN 73 378, Type: PA 12-HL.

Properties of compounds based on PA12 vary little with changing humidity due to low moisture absorption. Parts made of this semi-crystalline material are characterized by exceptional impact strength, low coefficient of friction and good chemical resistance.

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 
 

The values presented are typical or average values, they do not constitute a specification.
 
FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 25 / * cm³/10min ISO 1133
Temperatura 275 / * °C -
Carico 5 / * kg -
Ritiro di stampaggio, parallelo 0.7 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 1.3 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 1550 / 1300 MPa ISO 527
Carico unitario a trazione 46 / 42 MPa ISO 527
Deformazione a snervamento 4 / 12 % ISO 527
Deformazione nominale a rottura >50 / >50 % ISO 527
Resistenza all'urto Charpy, +23°C N / N kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C N / N kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 10 / 12 kJ/m² ISO 179/1eA
Type of failure C / C - -
Resistenzia all'urto Charpy con intaglio, -30°C 8 / 8 kJ/m² ISO 179/1eA
Type of failure C / C - -
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 178 / * °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 50 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 110 / * °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 140 / * °C ISO 306
Coeff.di dilatazione termica lin., parallelo 150 / * E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm HB / * class IEC 60695-11-10
Spessore provato 1.6 / * mm -
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 9.7 / 5 - IEC 62631-2-1
Costante dielettrica relativa, 1MHz 4 / 3.5 - IEC 62631-2-1
Fattore di dissipazione, 100Hz 2100 / 1000 E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 1100 / 500 E-4 IEC 62631-2-1
Resistività volumica 1E10 / 5E10 Ohm*m IEC 62631-3-1
Resistività superficiale * / 6E14 Ohm IEC 62631-3-2
Rigidità dielettrica 39 / 35 kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali 600 / 600 - IEC 60112
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 1.5 / * % Sim. alla ISO 62
Assorbimento d'umidità 0.7 / * % Sim. alla ISO 62
Massa volumica 1010 / 1020 kg/m³ ISO 1183
Preparazione ProvetteValoreUnitáNorma del test
ISO Data
Stamp. ad Iniezione, temp. di fusione 240 °C ISO 294
Stamp. ad Iniezione, temperatura dello stampo 60 °C ISO 294
Stamp. ad Iniezione, velocità media d'iniezione 200 mm/s ISO 294
Stamp. ad Iniezione, pressione di chiusura 70 MPa ISO 294
Funzioni
Sforzi-deformazione , VESTAMID® L2141 BK 9.7504 (Secco), PA12, Evonik
Modulo secante-deformazione , VESTAMID® L2141 BK 9.7504 (Secco), PA12, Evonik
Modulo a taglio-temperatura , VESTAMID® L2141 BK 9.7504 (Secco), PA12, Evonik
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Estrusione di tubi, Estrusione Profilati, Altre Estrusioni
Forma fisica disponibile
Pellet, Nero
Additivi
Lubrificanti
Caratteristiche speciali
Alto urto o modificato all'urto, Stabilizzato o stabile al calore
Caratteristiche
Grado tribologico
Resistenza Chimica
Resistenza chimica generale
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.