Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® LX9013 BK 9.7507 - PA12-I - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® LX9013 BK 9.7507:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto

High-viscosity, plasticized compound for extrusion with an extraordinary long-term heat resistance

VESTAMID® LX9013 BK 9.7507 is a plasticized polyamide 12 compound with an especially high long-term resistance under thermal load.

The material absorbs only little moisture, thus leading to nearly unaffected dimensions and properties of the finished parts at changing ambient conditions. Extruded tubes are impact-resistant also at low temperatures.

VESTAMID® LX9013 BK 9.7507 is suited to produce flexible tubes that are permanently exposed to higher temperatures, e.g., in the engine compartment of motor vehicles. Especially when used as diesel fuel lines they show significant advantages compared with standard grades, obvious in storage tests with diesel fuel (see the figure).

The material corresponds to the extrusion compound PA12-HIPHL, grade1 acc. DIN 73378 and meets the requirements acc. DIN 74324 (black), ISO 7628 and SAE J844.

VESTAMID® LX9013 BK 9.7507 is supplied as pellets in moisture-proof packaging ready for processing.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Ritiro di stampaggio, parallelo 0.4 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 1.5 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 410 / 400 MPa ISO 527
Resistenza all'urto Charpy, +23°C N / N kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C N / N kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 130 / 140 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 7 / 20 kJ/m² ISO 179/1eA
Type of failure C / C - -
Durezza Shore D 65 / * - ISO 7619-1
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 172 / * °C ISO 11357-1/-3
Temperatura di transizione vetrosa, 10°C/min 0 / * °C ISO 11357-1/-2
Temp.di inflessione sotto carico, 1.80 MPa 55 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 130 / * °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 130 / * °C ISO 306
Coeff.di dilatazione termica lin., parallelo 160 / * E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 160 / * E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm HB / * class IEC 60695-11-10
Spessore provato 1.6 / * mm -
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 12 / 15.6 - IEC 62631-2-1
Costante dielettrica relativa, 1MHz 3.4 / 3.6 - IEC 62631-2-1
Fattore di dissipazione, 100Hz 5000 / 6650 E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 1000 / 1390 E-4 IEC 62631-2-1
Resistività volumica 1E8 / 5.1E7 Ohm*m IEC 62631-3-1
Rigidità dielettrica 25 / 23 kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali 600 / - - IEC 60112
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 1.5 / * % Sim. alla ISO 62
Assorbimento d'umidità 0.6 / * % Sim. alla ISO 62
Massa volumica 1020 / 1020 kg/m³ ISO 1183
Caratteristiche
Processabilità e Forma di Forni
Estrusione di tubi, Estrusione Profilati, Altre Estrusioni
Forma fisica disponibile
Pellet, Nero
Additivi
Plastificante
Caratteristiche speciali
Alto urto o modificato all'urto, Stabilizzato o stabile al calore
Disponibilità geografica
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.