Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® LX9041 BK 9.7504 - PA12 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® LX9041 BK 9.7504:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Medium-viscosity, heat and light stabilized polyamide 12 compound

VESTAMID® LX9041 BK 9.7504 s a heat stabilized and light resistant polyamide 12 compound especially developed for extrusion coating of steel tubes.
 
Due to the exceptional impact strength, abrasion resistance and good chemical resistance of PA 12 as well as the excellent adhesion between the steel and the properly applied VESTAMID® LX9041 BK 9.7504 , the corrosion resistance of steel tubes coated with VESTAMID® LX9041 black is significantly increased.

VESTAMID® LX9041 BK 9.7504 is supplied as cylindrical granules, ready for processing, in moisture-proof bags.

The use of colorants may affect property values. 

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 17 / * cm³/10min ISO 1133
Temperatura 240 / * °C -
Carico 2.16 / * kg -
Ritiro di stampaggio, parallelo 1.1 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 1.1 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 1730 / 1370 MPa ISO 527
Carico unitario a trazione 51 / 44 MPa ISO 527
Deformazione a snervamento 4 / 12 % ISO 527
Deformazione nominale a rottura >50 / >50 % ISO 527
Resistenza all'urto Charpy, +23°C N / N kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C N / N kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 4 / 3.5 kJ/m² ISO 179/1eA
Type of failure C / C - -
Resistenzia all'urto Charpy con intaglio, -30°C 4.3 / 4 kJ/m² ISO 179/1eA
Type of failure C / C - -
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 177 / * °C ISO 11357-1/-3
Temperatura di transizione vetrosa, 10°C/min 44 / * °C ISO 11357-1/-2
Temp.di inflessione sotto carico, 1.80 MPa 48 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 120 / * °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 141 / * °C ISO 306
Reaz. al fuoco spess.nom. 1.5mm HB / * class IEC 60695-11-10
Spessore provato 1.6 / * mm -
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 3.7 / 4.4 - IEC 62631-2-1
Costante dielettrica relativa, 1MHz 3.1 / 3.2 - IEC 62631-2-1
Fattore di dissipazione, 100Hz 330 / 610 E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 195 / 363 E-4 IEC 62631-2-1
Resistività volumica 9.3E12 / 4.9E12 Ohm*m IEC 62631-3-1
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 1.3 / * % Sim. alla ISO 62
Assorbimento d'umidità 0.7 / * % Sim. alla ISO 62
Massa volumica 1020 / - kg/m³ ISO 1183
Preparazione ProvetteValoreUnitáNorma del test
ISO Data
Stamp. ad Iniezione, temp. di fusione 240 °C ISO 294
Stamp. ad Iniezione, temperatura dello stampo 60 °C ISO 294
Stamp. ad Iniezione, velocità media d'iniezione 200 mm/s ISO 294
Caratteristiche
Processabilità e Forma di Forni
Rivestimento
Forma fisica disponibile
Pellet, Nero
Caratteristiche speciali
Alto urto o modificato all'urto, Stabilizzato o stabile alla luce, Stabilizzato o stabile al calore
Caratteristiche
Buona adesione
Resistenza Chimica
Resistenza chimica generale
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com