Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® LX9012 - PA12 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® LX9012:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Heat stabilized and light resistant polyamide 12 compound

VESTAMID® LX9012 has been especially developed for the extrusion and co-extrusion of ski upper and decorative films. Decoration on the bottom side of injection molded sports shoe soles is a further application field.

Films made of VESTAMID® LX9012 feature high transparency, good screen and sublimation printing, outstanding scratch resistance, and excellent impact strength at low temperatures. The semi-crystalline compounds based on PA 12 absorb only low quantities of water.

Therefore, molded parts show excellent dimensional stability, constantly high impact strength, low coefficient of friction and good chemical resistance at changing ambient humidity. VESTAMID® LX9012 is supplied as cylindrical granules, ready for processing in moisture-proof packaging.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Ritiro di stampaggio, parallelo 1.3 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 1.3 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 1100 / - MPa ISO 527
Carico unitario a trazione 34 / - MPa ISO 527
Deformazione a snervamento 5 / - % ISO 527
Deformazione nominale a rottura >50 / - % ISO 527
Resistenza all'urto Charpy, +23°C N / - kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C N / - kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 13 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Resistenzia all'urto Charpy con intaglio, -30°C 15 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Durezza Shore D 71 / * - ISO 7619-1
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 176 / * °C ISO 11357-1/-3
Temperatura di transizione vetrosa, 10°C/min 39 / * °C ISO 11357-1/-2
Temp.di inflessione sotto carico, 1.80 MPa 45 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 120 / * °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 130 / * °C ISO 306
Coeff.di dilatazione termica lin., parallelo 130 / * E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 125 / * E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm HB / * class IEC 60695-11-10
Spessore provato 1.6 / * mm -
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 3.8 / - - IEC 62631-2-1
Costante dielettrica relativa, 1MHz 3 / - - IEC 62631-2-1
Fattore di dissipazione, 100Hz 530 / - E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 280 / - E-4 IEC 62631-2-1
Resistività volumica 1E12 / - Ohm*m IEC 62631-3-1
Res. Alle correnti striscianti superficiali 575 / - - IEC 60112
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 1.5 / * % Sim. alla ISO 62
Assorbimento d'umidità 0.8 / * % Sim. alla ISO 62
Massa volumica 1010 / - kg/m³ ISO 1183
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Estrusione Film, Estrusione Profilati, Altre Estrusioni
Forma fisica disponibile
Pellet
Caratteristiche speciali
Alto urto o modificato all'urto, Stabilizzato o stabile alla luce, Stabilizzato o stabile al calore, Trasparente
Caratteristiche
Resistente ai graffi, Grado tribologico
Resistenza Chimica
Resistenza chimica generale
Applicazioni
Attrezzature sportive
Disponibilità geografica
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com