Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTODUR® X7212 NC - PBT-GF45 FR(17) - Evonik Operations GmbH

Material Data Center offers the following functions for VESTODUR® X7212 NC:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestodur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Glass Fiber Reinforced and Flame Retardant Polybutylene Terephthalate Molding Compound 

VESTODUR® X7212 NC is a glass fiber-reinforced (45%), semi-crystalline thermoplastic com­pound for injection molding, based on polybutylene terephthalate (PBT). The self-extinguishing compound has a creamy-white colour.

 

VESTODUR® X7212 NC is used for parts of high mechanical and thermal resistance. 

 

Test bars made of the compound are rated V-0 self-extinguishing according to UL94 by Underwriters Laboratories Inc.

 

The incorporated flame retardant is non-migrating. The additive has no corrosive effects on metal inserts or neighboring metal parts. Therefore, the compound is distinguished for moldings in the electrical and electronical industry. Laser marking with high contrasts is possible.

 

VESTODUR® X7212 is supplied as cylindrical pellets in polyethylene packaging. 

 

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at tempIeratures not exceeding 30°C.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM 
OR VISIT OUR PRODUCT AT WWW.VESTODUR.COM

Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 8 / * cm³/10min ISO 1133
Temperatura 250 / * °C -
Carico 2.16 / * kg -
Ritiro di stampaggio, parallelo 0.2 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.7 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 15500 / 16100 MPa ISO 527
Carico unitario a rottura 145 / 150 MPa ISO 527
Deformazione a rottura 1.3 / 1.3 % ISO 527
Resistenza all'urto Charpy, +23°C 48 / 44 kJ/m² ISO 179/1eU
Type of failure C / C - -
Resistenza all'urto Charpy, -30°C 45 / 50 kJ/m² ISO 179/1eU
Type of failure C / C - -
Resistenzia all'urto Charpy con intaglio, +23°C 12 / 11 kJ/m² ISO 179/1eA
Type of failure C / C - -
Resistenzia all'urto Charpy con intaglio, -30°C 12 / 15 kJ/m² ISO 179/1eA
Type of failure C / C - -
Durezza Shore D 86 / * - ISO 7619-1
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 223 / * °C ISO 11357-1/-3
Temperatura di transizione vetrosa, 10°C/min 45 / * °C ISO 11357-1/-2
Temp.di inflessione sotto carico, 1.80 MPa 217 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 223 / * °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 215 / * °C ISO 306
Coeff.di dilatazione termica lin., parallelo 20 / * E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 40 / * E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm V-0 / * class IEC 60695-11-10
Spessore provato 1.5 / * mm -
Reazione al fuoco a spessore h V-0 / * class IEC 60695-11-10
Spessore provato 0.8 / * mm -
Indice di ossigeno 37 / * % ISO 4589-1/-2
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 4.4 / - - IEC 62631-2-1
Costante dielettrica relativa, 1MHz 4.6 / - - IEC 62631-2-1
Fattore di dissipazione, 100Hz 40 / - E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 130 / - E-4 IEC 62631-2-1
Resistività superficiale * / 1E13 Ohm IEC 62631-3-2
Res. Alle correnti striscianti superficiali 275 / - - IEC 60112
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 0.3 / * % Sim. alla ISO 62
Assorbimento d'umidità 0.1 / * % Sim. alla ISO 62
Massa volumica 1840 / - kg/m³ ISO 1183
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet, Colore naturale
Additivi
Agente di distacco
Caratteristiche speciali
Ritardante di fiamma, Stabilizzato o stabile alla luce, Stabilizzato o stabile al calore
Caratteristiche
Adatti alla marcatura laser
Applicazioni
Elettrotecnica ed electrici
Disponibilità geografica
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.