Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Vydyne® 22HSP NT - PA66 - Ascend

Material Data Center offers the following functions for Vydyne® 22HSP NT:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vydyne datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Vydyne 22HSP NT is a general-purpose, unfilled, lubricated, heat stabilized PA66 resin. Designed principally for injection-molding fabrication, this product offers a combination of engineering properties characterized by high strength; rigidity; good toughness; high melt point; good surface lubricity; abrasion resistance; and resistance to many chemicals, machine and motor oils, solvents and gasoline. This product is designed to resist thermal degradation when exposed to warm climates.
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Ritiro di stampaggio, parallelo 2.2 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 2.0 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 2900 / 1700 MPa ISO 527
Carico unitario a trazione 85 / 55 MPa ISO 527
Deformazione a snervamento 5 / 20 % ISO 527
Carico unitario a rottura 55 / 40 MPa ISO 527
Deformazione a rottura 25 / >50 % ISO 527
Modulo a flessione, 23°C 2900 / 1000 MPa ISO 178
Resistenza alla flessione 95 / 30 MPa ISO 178
Resistenza all'urto Charpy, +23°C N / N kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C N / N kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 3.7 / 8.6 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 3.4 / 3 kJ/m² ISO 179/1eA
Resistenza all'urto Izod con intaglio, +23°C 6 / 20 kJ/m² ISO 180/1A
Resistenza all'urto Izod con intaglio 5 / 7 kJ/m² ISO 180/1A
Temperatura -30 °C -
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 260 / * °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 67 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 179 / * °C ISO 75-1/-2
Coeff.di dilatazione termica lin., parallelo 100 / * E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin. , perpend. 100 / * E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm V-2 / * class IEC 60695-11-10
Spessore provato 1.5 / * mm -
Reazione al fuoco a spessore h V-2 / * class IEC 60695-11-10
Spessore provato 0.7 / * mm -
Indice di ossigeno 24 / * % ISO 4589-1/-2
Glow Wire Flammability Index (GWFI) 825 °C IEC 60695-2-12
GWFI - thickness tested (1) 0.71 mm -
Glow Wire Flammability Index (GWFI) 825 °C IEC 60695-2-12
GWFI - thickness tested (2) 1.5 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (3) 3 mm -
Glow Wire Ignition Temperature (GWIT) 700 °C IEC 60695-2-13
GWIT - thickness tested (1) 0.71 mm -
Glow Wire Ignition Temperature (GWIT) 700 °C IEC 60695-2-13
GWIT - thickness tested (2) 1.5 mm -
Glow Wire Ignition Temperature (GWIT) 700 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
ASTM Data
UL 94 combustibilitá V-2 - UL 94
Spessore testati 0.71 mm -
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Resistività volumica 1E16 / - Ohm*m IEC 62631-3-1
Rigidità dielettrica 29 / - kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali 500 / - - IEC 60112
ASTM Data
Resistenza all’arco 90 / - s ASTM D 495
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 2.4 / * % Sim. alla ISO 62
Massa volumica 1140 / - kg/m³ ISO 1183
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 70 °C -
Pre-essiccamento - Tempo 1 - 3 h -
Temperatura di fusione 285 - 300 °C -
Temperatura dello stampo 65 - 95 °C -
Zona 1 260 - 280 °C -
Zona 2 270 - 285 °C -
Zona 3 280 - 290 °C -
Temperatura dell ugello 280 - 300 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet, Colore naturale
Additivi
Lubrificanti, Agente di distacco
Caratteristiche speciali
Stabilizzato o stabile al calore
Resistenza Chimica
Resistenza chimica generale, Resistenza ai solventi, Resistenza all’olio
Certifications
Contatto con gli alimenti, Approvato per l'utilizzo per contatto con alimenti secondo la FDA 21 CFR, Contatto con acqua potabile, Contatto con acqua potabile NSF 61
Applicazioni
Automotive, Elettrotecnica ed electrici, Polivalente
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.