Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Vydyne® ECO366H BK0734 - PA66 - Ascend

Material Data Center offers the following functions for Vydyne® ECO366H BK0734:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Vydyne datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Carico unitario a trazione 83 / - MPa ISO 527
Deformazione a rottura 4 / - % ISO 527
Modulo a flessione, 23°C 3900 / - MPa ISO 178
Resistenza alla flessione 107 / - MPa ISO 178
Resistenza all'urto Charpy, +23°C 75 / - kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C 78 / - kJ/m² ISO 179/1eU
Resist. urto Charpy con intaglio, +23°C 3.4 / - kJ/m² ISO 179/1eA
Resist. urto Charpy con intaglio, -30°C 3.7 / - kJ/m² ISO 179/1eA
Resistenza all'urto Izod, +23°C 6 / - kJ/m² ISO 180/1U
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 265 / * °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 75 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 240 / * °C ISO 75-1/-2
Reaz. al fuoco spess.nom. 1.5mm V-0 / * class IEC 60695-11-10
Spessore provato 1.5 / * mm -
Reazione al fuoco a spessore h V-0 / * class IEC 60695-11-10
Spessore provato 0.4 / * mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (1) 0.4 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (2) 0.75 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (3) 1.5 mm -
Glow Wire Ignition Temperature (GWIT) 960 °C IEC 60695-2-13
GWIT - thickness tested (1) 0.4 mm -
Glow Wire Ignition Temperature (GWIT) 960 °C IEC 60695-2-13
GWIT - thickness tested (2) 0.75 mm -
Glow Wire Ignition Temperature (GWIT) 800 °C IEC 60695-2-13
GWIT - thickness tested (3) 1.5 mm -
ASTM Data
UL 94 combustibilitá V-0 - UL 94
Spessore testati 0.4 mm -
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Resistività volumica 1E8 / - Ohm*m IEC 62631-3-1
Rigidità dielettrica 17 / - kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali 600 / - - IEC 60112
ASTM Data
Resistenza all’arco 150 / - s ASTM D 495
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 80 °C -
Pre-essiccamento - Tempo 4 h -
Temperatura di fusione 270 - 285 °C -
Temperatura dello stampo 65 - 95 °C -
Zona 1 260 - 290 °C -
Zona 2 260 - 290 °C -
Zona 3 260 - 290 °C -
Temperatura dell ugello 260 - 290 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Nero
Additivi
Lubrificanti, Agente di distacco
Caratteristiche speciali
Ritardante di fiamma, Senza alogeni, Stabilizzato o stabile al calore
Caratteristiche
Stabilità termica, Omopolimero
Resistenza Chimica
Resistenza chimica generale
Applicazioni
Automotive, Elettrotecnica ed electrici
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.