Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Vydyne® R535J BK0678 - PA66-GF35 - Ascend

Material Data Center offers the following functions for Vydyne® R535J BK0678:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vydyne datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Vydyne R535J BK0678 is a black, 35% glass filled, high flow, PA66 that contains an electrically neutral heat stabilizer. It is specifically designed for electrical applications requiring high dielectric strength, low conductivity, corrosion resistance, and laser markability.
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Ritiro di stampaggio, parallelo 0.4 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.9 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 11600 / - MPa ISO 527
Carico unitario a rottura 209 / - MPa ISO 527
Deformazione a rottura 2.8 / - % ISO 527
Modulo a flessione, 23°C 10500 / - MPa ISO 178
Resistenza alla flessione 300 / - MPa ISO 178
Resistenza all'urto Charpy, +23°C 79 / - kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C 68 / - kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 12 / - kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 11 / - kJ/m² ISO 179/1eA
Resistenza all'urto Izod con intaglio, +23°C 12 / - kJ/m² ISO 180/1A
Resistenza all'urto Izod con intaglio 11 / - kJ/m² ISO 180/1A
Temperatura -30 °C -
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 260 / * °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 251 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 261 / * °C ISO 75-1/-2
Coeff.di dilatazione termica lin., parallelo 21 / * E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 106 / * E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm HB / * class IEC 60695-11-10
Spessore provato 1.5 / * mm -
Reazione al fuoco a spessore h HB / * class IEC 60695-11-10
Spessore provato 0.8 / * mm -
Glow Wire Flammability Index (GWFI) 750 °C IEC 60695-2-12
GWFI - thickness tested (1) 0.75 mm -
Glow Wire Flammability Index (GWFI) 725 °C IEC 60695-2-12
GWFI - thickness tested (2) 1.5 mm -
Glow Wire Flammability Index (GWFI) 800 °C IEC 60695-2-12
GWFI - thickness tested (3) 3 mm -
Glow Wire Ignition Temperature (GWIT) 775 °C IEC 60695-2-13
GWIT - thickness tested (1) 0.75 mm -
Glow Wire Ignition Temperature (GWIT) 725 °C IEC 60695-2-13
GWIT - thickness tested (2) 1.5 mm -
Glow Wire Ignition Temperature (GWIT) 750 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
ASTM Data
UL 94 combustibilitá HB - UL 94
Spessore testati 0.75 mm -
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Resistività volumica 1E12 / - Ohm*m IEC 62631-3-1
Rigidità dielettrica 27 / 20 kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali 600 / - - IEC 60112
ASTM Data
Resistenza all’arco 150 / - s ASTM D 495
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 0.8 / * % Sim. alla ISO 62
Assorbimento d'umidità 1.6 / * % Sim. alla ISO 62
Massa volumica 1410 / - kg/m³ ISO 1183
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 80 °C -
Pre-essiccamento - Tempo 4 h -
Temperatura di fusione 285 - 305 °C -
Temperatura dello stampo 65 - 95 °C -
Zona 1 280 - 310 °C -
Zona 2 280 - 310 °C -
Zona 3 280 - 310 °C -
Temperatura dell ugello 280 - 310 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet, Nero
Additivi
Lubrificanti, Agente di distacco
Caratteristiche speciali
Stabilizzato o stabile al calore
Caratteristiche
Adatti alla marcatura laser
Resistenza Chimica
Resistenza chimica generale
Applicazioni
Automotive, Elettrotecnica ed electrici
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.