Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of XAREC® EA 522 - (PS-SY)-GF22 - Idemitsu Chemicals

Material Data Center offers the following functions for XAREC® EA 522:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Xarec datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
Other Standards[S]
Ritiro di stampaggio, parallelo 0.3 % Producer Method
Ritiro di stampaggio, perpendicolare 0.6 % Producer Method
S: These properties are reported by the producer according standards that are different to our defaults.
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 8000 MPa ISO 527
Carico unitario a rottura 100 MPa ISO 527
Deformazione a rottura 2.3 % ISO 527
Modulo a flessione, 23°C 7500 MPa ISO 178
Resistenza alla flessione 155 MPa ISO 178
Resistenza all'urto Charpy, +23°C 39 kJ/m² ISO 179/1eU
Resist. urto Charpy con intaglio, +23°C 12 kJ/m² ISO 179/1eA
Resistenza all'urto Izod, +23°C 34 kJ/m² ISO 180/1U
Resistenza all'urto Izod con intaglio, +23°C 11 kJ/m² ISO 180/1A
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 230 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 265 °C ISO 75-1/-2
Coeff.di dilatazione termica lin., parallelo 24 E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin. , perpend. 53 E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm V-0 class IEC 60695-11-10
Spessore provato 1.5 mm -
Yellow Card disponibile - -
Reazione al fuoco 5V a spess. h 5VA class IEC 60695-11-20
Spessore provato 2.2 mm -
Yellow Card disponibile - -
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Res. Alle correnti striscianti superficiali 500 - IEC 60112
ASTM Data
Rigidità elettrica, breve periodo di tempo 35 kV/mm ASTM D 149
Resistenza all’arco 150 s ASTM D 495
Other Standards[S]
Costante dielettrica relativa, 1MHz 3 - IEC 60250
Fattore di dissipazione, 1MHz 10 E-4 IEC 60250
Resistività volumica 1E14 Ohm*m IEC 60093
S: These properties are reported by the producer according standards that are different to our defaults.
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'umidità 0.01 % Sim. alla ISO 62
Massa volumica 1320 kg/m³ ISO 1183
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 120 °C -
Pre-essiccamento - Tempo 3 - 5 h -
Temperatura di fusione 280 - 310 °C -
Temperatura dello stampo 130 - 155 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet
Caratteristiche speciali
Ritardante di fiamma, Alto urto o modificato all'urto
Applicazioni
Elettrotecnica ed electrici
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.