Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Badaflex® TPE-S 50A 1659 2K - SEBS - Bada AG

Material Data Center offers the following functions for Badaflex® TPE-S 50A 1659 2K:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Badaflex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Deformazione residua dopo compressione a 70°C, 24h 58 % ISO 815
Resistenza alla lacerazione 22 kN/m ISO 34-1
Durezza Shore A 50 - ISO 7619-1
Other Standards[S]
Resistenza a trazione 6 MPa DIN 53504
Allungamento a rottura TPE 450 % DIN 53504
S: These properties are reported by the producer according standards that are different to our defaults.
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1160 kg/m³ ISO 1183
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 60 - 80 °C -
Pre-essiccamento - Tempo 2 - 4 h -
Umidità del Processo ≤0.1 % -
Temperatura di fusione 220 - 250 °C -
Temperatura dello stampo 60 - 80 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Caratteristiche speciali
Stabilizzato o stabile al calore
Caratteristiche
Buona adesione
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.